Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 28 cSt | 28 cSt | Base Oil; ASTM D445 |
Nye Lubricants 184M (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 28 cSt @Temperature 40.0 °C |
28 cSt @Temperature 104 °F |
ASTM D445 |
PolyOne Synplast™ DUP-E Di Undecyl Phthalate Linear C11 phthalate esterContains 0.10-0.15 wt% 1,1,3-Tris (2-methyl-4hydroxy-5-t-butyl phenyl) butane antioxidantInformation provided by PolyOne |
|||
Kinematic Viscosity at 40°C (104°F) | 28 cSt | 28 cSt | |
ChevronTexaco Cetus® DE 32 Texaco Cetus DE oils deliver value through:Long life — Texaco Cetus DE oils have a low sludge-forming tendency and a high solvency for deposits that help to keep compressor parts clean. Their abili.. |
|||
Kinematic Viscosity at 40°C (104°F) | 28 cSt | 28 cSt | |
ConocoPhillips 32 Soluble Oil Description: Conoco Soluble Oil is a general-purpose oil suited for a wide variety of cutting and grinding operations that require a combination water-soluble lubricant and coolant. Soluble Oil is a.. |