Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 145.2 cSt | 145.2 cSt | |
ChevronTexaco Thuban® SAE 80W-90 Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing. CPS Number: 220993; MSDS Number: 8801 |