Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 13 cSt | 13 cSt | ASTM D445 |
ExxonMobil Mobilarma 777 The Mobilarma 700 Series contains three premium performance rust preventives that cover a range of applications including storage and inter-operational activities. The Mobilarma 777 and 778 are inte.. |
|||
Kinematic Viscosity at 40°C (104°F) | 13 cSt | 13 cSt | ASTM D445 |
ChevronTexaco Superla® DCO FeaturesChevron Superla DCO is a highly refined food grade white mineral oil that exceeds FDA purity requirements for the dedusting of grains intended for human consumption.Chevron Superla DCO conta.. |
|||
Kinematic Viscosity at 40°C (104°F) | 13 cSt | 13 cSt | |
ChevronTexaco Transultex® CF A Texaco Transultex CF metalworking fluids deliver value through:Excellent antiweld properties from active sulfur and chlorine-free EP compounding which reduce frictional heat, prevent welding of meta.. |
|||
Kinematic Viscosity at 40°C (104°F) | 13 cSt | 13 cSt | ASTM D445 |
ExxonMobil Mobilarma 777 The Mobilarma 700 Series contains three premium performance rust preventives that cover a range of applications including storage and inter-operational activities. The Mobilarma 777 and 778 are inte.. |
|||
Kinematic Viscosity at 40°C (104°F) | 13 cSt | 13 cSt | |
ChevronTexaco Alcaid® 13 Texaco Alcaid® oils deliver value through:Low pour points that permit oils to remain fluid at subzero temperatures.Ready separation from water, an important property where severe moisture condition.. |