Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 112 cSt | 112 cSt | ASTM D445 |
ExxonMobil SAE 30 Mobilgard M30 Series Mobilgard M30 Series (M330 and M430) by ExxonMobil are premium, extra high performance 30 TBN engine oils designed for use in the most severe residual-fueled, medium-speed diesel engines used in mar.. |
|||
Kinematic Viscosity at 40°C (104°F) | 112 cSt | 112 cSt | ASTM D445 |
ExxonMobil SAE 30 Mobilgard M30 Series Mobilgard M30 Series (M330 and M430) by ExxonMobil are premium, extra high performance 30 TBN engine oils designed for use in the most severe residual-fueled, medium-speed diesel engines used in mar.. |
|||
Kinematic Viscosity at 40°C (104°F) | 112 cSt | 112 cSt | |
ChevronTexaco Doro® AR SAE 30 Texaco Doro AR delivers value through:Wear protection — Contains alkaline reserves which protect against acids formed by combustion.Cleanliness — Detergent properties ensure a clean Crankcase, pis.. |
|||
Kinematic Viscosity at 40°C (104°F) | 112 cSt | 112 cSt | ASTM D445 |
ChevronTexaco Dura-Lith® NLGI 0 Grease EP FeaturesChevron Dura-Lith Greases EP are multipurpose extreme pressure greases.They are manufactured using selected highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thic.. |
|||
Kinematic Viscosity at 40°C (104°F) | 112 cSt | 112 cSt | ASTM D445 |
ChevronTexaco Dura-Lith® NLGI 00 Grease EP FeaturesChevron Dura-Lith Greases EP are multipurpose extreme pressure greases.They are manufactured using selected highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thic.. |