Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 100°F | 39.2 SUS | 39.2 SUS | |
Heatbath/Park Plastiquench Water-Based Quenchant A solution of polyvinyl alcohol in water, used as a base for steel quenching media. In water solution, it cools austenitized steels faster then quenching oils, hardens steels with less distortion or.. |