Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 100°F | 800 SUS | 800 SUS | |
Lubriplate 730-0 Aluminum Complex Multi-Purpose Grease High performance aluminum complex greases that provide high load carrying ability and AW protection with high resistance to water, steam, and other corrosive action. Available in 3 NLGI densities fo.. |
|||
Saybolt Viscosity at 100°F | 800 SUS | 800 SUS | |
Lubriplate 730-1 Aluminum Complex Multi-Purpose Grease High performance aluminum complex greases that provide high load carrying ability and AW protection with high resistance to water, steam, and other corrosive action. Available in 3 NLGI densities fo.. |
|||
Saybolt Viscosity at 100°F | 800 SUS | 800 SUS | |
Lubriplate 730-2 Aluminum Complex Multi-Purpose Grease High performance aluminum complex greases that provide high load carrying ability and AW protection with high resistance to water, steam, and other corrosive action. Available in 3 NLGI densities fo.. |
|||
Saybolt Viscosity at 100°F | 800 SUS | 800 SUS | |
Lubriplate 630-AAA Lithium Based Multi-Purpose Grease These popular lithium type greases are excellent for a wide range of lubrication demands thus reducing the need to carry large grease inventories. They show exceptional resistance to water, steam, a.. |