Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Gravity = 0.863 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Specific Gravity 0.863 g/cc
0.863 g/cc
15°C; ASTM D1298
ExxonMobil 220 Mobil SHC PM Series
Mobil SHC PM Series products are supreme performance synthetic lubricants specifically designed for the most demanding industrial paper machine circulating systems. They are engineered to provide ex..
Specific Gravity 0.863 g/cc
0.863 g/cc
15.6°C; ASTM D4052
ExxonMobil 460 Mobilgear SHC XMP Series
Mobilgear SHC XMP Series supreme performance, fully synthetic industrial gear oils designed to provide optimum equipment protection and oil life even under extreme conditions. Mobil polyalphaolefin ..
Specific Gravity 0.863 g/cc
0.863 g/cc
ASTM D1505
ExxonMobil Vistamaxx™ 6202 Propylene-based Elastomer
Product Description: Vistamaxx 6202 propylene-based elastomer is an olefinic elastomer produced using ExxonMobil Chemical's EXXPOL™ Catalyst Technology. It has excellent elastomeric properties, i..
Specific Gravity 0.863 g/cc
0.863 g/cc
ASTM D1505
ExxonMobil Vistamaxx™ 6202FL Propylene-based Elastomer - Performance Film
Product Description: Vistamaxx 6202FL propylene-based elastomer is an olefinic elastomer primarily composed of isostatic propylene repeat units with random ethylene distribution, and is produced us..
Specific Gravity 0.863 g/cc
0.863 g/cc
15°C; ASTM D1298
ExxonMobil 220 Mobil SHC PM Series
Mobil SHC PM Series products are supreme performance synthetic lubricants specifically designed for the most demanding industrial paper machine circulating systems. They are engineered to provide ex..
Specific Gravity 0.863 g/cc
0.863 g/cc
ChevronTexaco Superla® 21 White Oil
FeaturesChevron Superla White Oils are colorless, odorless, tasteless mixtures of saturated paraffinic and naphthenic hydrocarbons that span a viscosity range of 50-625 SUS at 100°F.These nearly ch..
Specific Gravity 0.863 g/cc
0.863 g/cc
15.6°C; ASTM D4052
ExxonMobil 460 Mobilgear SHC XMP Series
Mobilgear SHC XMP Series supreme performance, fully synthetic industrial gear oils designed to provide optimum equipment protection and oil life even under extreme conditions. Mobil polyalphaolefin ..
Copyright © lookpolymers.com All Rights Reserved