Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 4.20 - 4.30 g/cc | 4.20 - 4.30 g/cc | |
Reade Advanced Materials Ilmenite Powder (FeTiO3) Description: A naturally mined iron titanium oxide mineral. It is generally black as sand, odorless, tasteless, opaque under a microscope, non-flammable and insoluble at 20 deg. C. Physical Properti.. |