Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.45 - 2.50 g/cc | 2.45 - 2.50 g/cc | |
Potters Industries Ballotini® Impact Beads Ballotini® impact beads are microspheres are used for precise metal finishing of parts. They offer an environmentally safe and cost effective method for metal surface cleaning and finishing. Coars.. |