Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.65 - 2.15 g/cc | 1.65 - 2.15 g/cc | Base Material; ASTM D792 |
Parker Chomerics CHO-SEAL 1285R Reinforced Conductive Elastomer Seal These materials are fabric-reinforced, silver-plated-aluminum filled EMI seals for airframe shielding applications. These seal materials can also be used to maintain surface electrical continuity at.. |
|||
Specific Gravity | 1.65 - 2.15 g/cc | 1.65 - 2.15 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL 1350 Conductive Elastomer Standard material for high volume injection and compression molding and small extrusions; high performance in non-corrosive environments; used in grounding applications with little or no vibration.R.. |
|||
Specific Gravity | 1.65 - 2.15 g/cc | 1.65 - 2.15 g/cc | |
Parker Chomerics CHO-SEAL E6306 Conductive Elastomer Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics |
|||
Specific Gravity | 1.65 - 2.15 g/cc | 1.65 - 2.15 g/cc | |
Parker Chomerics CHO-SEAL S6304 Conductive Elastomer Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics |
|||
Specific Gravity | 1.95 - 2.15 g/cc | 1.95 - 2.15 g/cc | ISO 1183 |
Raschig Group RALUPOL® 5000 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, excellent heat resistance, good mechanical strength. This product meets the all.. |
|||
Specific Gravity | 1.65 - 2.15 g/cc | 1.65 - 2.15 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL® 6307 Conductive Elastomer Description: Good performance in moderately corrosive environments; excellent NBC fluid resistance; good physical properties.Molded onlyRoHS CompliantInformation provided by Chomerics |
|||
Specific Gravity | 2.09 - 2.15 g/cc | 2.09 - 2.15 g/cc | ASTM D 792 |
Karina 1100/1075 IE MBPP White Color Concentrate Filled white concentrate recommended for olefin applications. Recommended usage from 5%.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |