Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.70 - 1.86 g/cc | 1.70 - 1.86 g/cc | ASTM D792 |
Daikin NEOFLON EP-521 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Specific Gravity | 1.70 - 1.86 g/cc | 1.70 - 1.86 g/cc | ASTM D792 |
Daikin NEOFLON EP-610 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Specific Gravity | 1.70 - 1.86 g/cc | 1.70 - 1.86 g/cc | ASTM D792 |
Daikin NEOFLON EP-610AS ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Specific Gravity | 1.70 - 1.86 g/cc | 1.70 - 1.86 g/cc | ASTM D792 |
Daikin NEOFLON EP-620 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Specific Gravity | 1.70 - 1.86 g/cc | 1.70 - 1.86 g/cc | ASTM D792 |
Daikin NEOFLON EP-541 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |