Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.45 - 1.75 g/cc | 1.45 - 1.75 g/cc | |
Parker Chomerics CHO-SHIELD® 610 A/B Epoxy Conductive Coating Description: CHO-SHIELD® 610 A/B is a highly conductive, two-component silver-plated-copper filled epoxy coating for application to non-conductive plastic substrates, particularly those subject to .. |
|||
Specific Gravity | 1.65 - 1.75 g/cc | 1.65 - 1.75 g/cc | ISO 1183 |
Raschig Group AMPLA® 7250 melamine-modified polyester Cellulose reinforced melamine-modified Polyester molding compound. Very good electrical values, excellent heat resistance, excellent surface quality, low post shrinkage. This product meets the allow.. |
|||
Specific Gravity | 1.60 - 1.75 g/cc | 1.60 - 1.75 g/cc | ISO 1183 |
Raschig Group DECAL® 1760 Phenolic Glass-fiber reinforced phenolic molding compound. Very good electrical properties, good chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals an.. |
|||
Specific Gravity | 1.65 - 1.75 g/cc | 1.65 - 1.75 g/cc | ISO 1183 |
Raschig Group DECAL® 937 Phenolic Mica reinforced phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 2002/96 (W.. |
|||
Specific Gravity | 1.60 - 1.75 g/cc | 1.60 - 1.75 g/cc | ISO 1183 |
Raschig Group MELOPLAS® 2500 MF Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al.. |
|||
Specific Gravity | 1.70 - 1.75 g/cc | 1.70 - 1.75 g/cc | ASTM D792 |
Mar-Bal MB2000-25 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Specific Gravity | 1.25 - 1.75 g/cc | 1.25 - 1.75 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL® 2532 Non-Conductive Extruded Elastomer Specifications Description: Chomerics manufactures a dual performance extruded gasket in one simple design. By a seam vulcanization process, CHO-SEAL conductive elastomers are extruded in parallel with non-conduct.. |
|||
Specific Gravity | 1.70 - 1.75 g/cc | 1.70 - 1.75 g/cc | ISO 12086 |
Isoflon ETFE Fluoropolymer material specifications.Information provided by Isoflon. |