Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.30 - 1.40 g/cc | 1.30 - 1.40 g/cc | ISO 1183 |
Raschig Group DECAL® 2061 Phenolic Wood flour reinforced phenolic molding compound. Good electrical properties, chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals and PCAs and .. |
|||
Specific Gravity | 1.35 - 1.40 g/cc @Thickness 1.57 mm |
1.35 - 1.40 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP842 Paper Base Laminate
(discontinued **) Description: Paper reinforced phenolic grade with controlled conductivity. Mechanical strength similar to NP611. NP842 is semi-conductive on the surfaces and through the laminate.Thickness Tested: 0.. |
|||
Specific Gravity | 1.35 - 1.40 g/cc @Thickness 1.57 mm |
1.35 - 1.40 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP310 Cotton Fabric Description: Canvas machining grade for structural and mechanical applications. Better impact strength than phenolic paper grades. MIL-I-24768/16. Thickness Tested: 0.062, 0.125", and 0.500". |
|||
Specific Gravity | 1.30 - 1.40 g/cc @Thickness 1.57 mm |
1.30 - 1.40 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP320U Cotton Fabric Description: Utility version of NP320E. Meets most, but not all, NEMA properties for L and LE, and is not certifiable as a NEMA Grade.Thickness Tested: 0.062", 0.125", and 0.500" |
|||
Specific Gravity | 1.30 - 1.40 g/cc @Thickness 1.57 mm |
1.30 - 1.40 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP310U Cotton Fabric Description: Utility grade canvas phenolic with properties similar to NP310E.Not certifiable to NEMA due to low crosswise flexural strength. Previously designated NP310C.Thickness Tested: 0.062", 0... |
|||
Specific Gravity | 1.35 - 1.40 g/cc @Thickness 1.57 mm |
1.35 - 1.40 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP612 Paper Base Laminate Description: Room temperature punching and shearing grade up to .125" thick. More flexible and lower mechanical properties than NP611. Intended for applications where electrical and moisture require.. |
|||
Specific Gravity | 1.30 - 1.40 g/cc @Thickness 1.57 mm |
1.30 - 1.40 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP664 Paper Base Laminate Description: Low cost room temperature punching grade with mechanical and electrical properties similar to NP612. This version is made with pigment cover plies on the surface.Thickness Tested: 0.062.. |
|||
Specific Gravity | 1.20 - 1.40 g/cc | 1.20 - 1.40 g/cc | IEC 1212-2 7.2 |
Hippe PF CC 32 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in mechanical, electrical and electronic applications. Coarse weave (18 to 30 threads per cm).Information provided by Hippe. |
|||
Specific Gravity | 1.20 - 1.40 g/cc | 1.20 - 1.40 g/cc | IEC 1212-2 7.2 |
Hippe PF CC 42 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in mechanical and electrical applications. Coarse weave (18 to 30 threads per cm).Information provided by Hippe. |
|||
Specific Gravity | 1.30 - 1.40 g/cc | 1.30 - 1.40 g/cc | IEC 1212-2 8.1 |
Hippe PF CP 201 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in mechanical applications. Used in mechanical properties better than other PF CP types. Poor electrical properties under normal humidity. Also available in hot-punching versions.Information.. |
|||
Specific Gravity | 1.30 - 1.40 g/cc | 1.30 - 1.40 g/cc | IEC 1212-2 8.1 |
Hippe PF CP 203 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in mechanical and electrical applications. Good electrical properties under normal humidity. Also available in hot-punching versions.Information provided by Hippe. |
|||
Specific Gravity | 1.30 - 1.40 g/cc | 1.30 - 1.40 g/cc | IEC 1212-2 8.1 |
Hippe PF CP 204 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in electrical and electronic applications. Good stability of electrical properties under high humidity. Also available in cold or hot-punching versions.Information provided by Hippe. |
|||
Specific Gravity | 1.30 - 1.40 g/cc | 1.30 - 1.40 g/cc | IEC 1212-2 8.1 |
Hippe PF CP 206 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in mechanical and electrical applications. Good electrical properties under normal humidity. Also available in hot-punching versions.Information provided by Hippe. |
|||
Specific Gravity | 1.30 - 1.40 g/cc | 1.30 - 1.40 g/cc | IEC 1212-2 8.1 |
Hippe PF CP 207 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in mechanical applications. Used in mechanical properties better than other PF CP types. Poor electrical properties under normal humidity. Also available in hot-punching versions. Improved .. |
|||
Specific Gravity | 1.30 - 1.40 g/cc | 1.30 - 1.40 g/cc | IEC 1212-2 8.1 |
Hippe PF CP 308 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in mechanical and electrical applications. Good electrical properties under normal humidity. Also available in hot-punching versions. Flame retardant.Information provided by Hippe. |
|||
Specific Gravity | 1.30 - 1.40 g/cc | 1.30 - 1.40 g/cc | IEC 1212-2 8.1 |
Hippe PF WV 304 Wood veneer Reinforced Phenolic Resin - Sheet Parallel plied. Used in mechanical and electrical applications.Information provided by Hippe. |
|||
Specific Gravity | 1.30 - 1.40 g/cc | 1.30 - 1.40 g/cc | IEC 1212-2 8.1 |
Hippe PF CC 201 Woven Cotton Cloth Reinforced Phenolic Resin - Sheet Used in mechanical applications (coarse weave: >130 g/m2, =30 threads/cm). Better mechanical properties and poorer electrical properties than type PF CC 202.Information provided by Hippe. |
|||
Specific Gravity | 1.36 - 1.40 g/cc | 1.36 - 1.40 g/cc | ASTM D-792 |
Axiall 8820 Moldings & Extrusions Flexible PVC General purpose extrusion and molding compound designed for use in weatherstrips, screen spline and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 201.. |
|||
Specific Gravity | 1.36 - 1.40 g/cc | 1.36 - 1.40 g/cc | ASTM D-792 |
Axiall 15881 Wire & Cable Flexible PVC 80C general purpose. 300 hour sunlight resistant.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.36 - 1.40 g/cc | 1.36 - 1.40 g/cc | ASTM D-792 |
Axiall 8630 Moldings & Extrusions Flexible PVC Extrusion compound recommended for extruded shapes and other applications where a matte finish is desired.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.36 - 1.40 g/cc | 1.36 - 1.40 g/cc | ASTM D-792 |
Axiall 8800 Moldings & Extrusions Flexible PVC General purpose extrusion compound designed for use in weatherstrips, screen spline and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.36 - 1.40 g/cc | 1.36 - 1.40 g/cc | ASTM D-792 |
Axiall 8803 Moldings & Extrusions Flexible PVC Microbe resistant extrusion and molding compound designed for use in weatherstrips, screen spline and flexible gaskets. Good UV resistance.Information provided by Georgia GulfGeorgia Gulf became Ax.. |
|||
Specific Gravity | 1.36 - 1.40 g/cc | 1.36 - 1.40 g/cc | ASTM D-792 |
Axiall 10756 Wire & Cable Flexible PVC General purpose, non-lead stabilized jacketing compound recommended for a maximum service temperature of 80°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.36 - 1.40 g/cc | 1.36 - 1.40 g/cc | ASTM D-792 |
Axiall 2192 Wire & Cable Flexible PVC Non-lead stabilized SJTO, SJTOO oil resistant flexible cord jacket. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corpo.. |
|||
Specific Gravity | 1.36 - 1.40 g/cc | 1.36 - 1.40 g/cc | ASTM D792 |
Compuestos Dominicanos Polycom VN-051090 PVC Compound Compuestos Dominicanos SA manufactures polycom VN product series for the extrusion of printable sheets and banners providing excellent stability, ease of processing and excellent printable character.. |
|||
Specific Gravity | 1.20 - 1.40 g/cc | 1.20 - 1.40 g/cc | IEC 1212-2 7.2 |
Hippe PF CP 43 Cellulose Paper Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in mechanical applications and low-voltage electrical applications.Information provided by Hippe. |
|||
Specific Gravity | 1.36 - 1.40 g/cc | 1.36 - 1.40 g/cc | ASTM D-792 |
Axiall 46234B Flexible PVC Injection molding compound designed for automotive encapsulation applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.36 - 1.40 g/cc | 1.36 - 1.40 g/cc | ASTM D-792 |
Axiall 8450 Moldings & Extrusions Flexible PVC High durometer, general purpose extrusion compound formulated for microbial resistance.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.36 - 1.40 g/cc | 1.36 - 1.40 g/cc | ASTM D-792 |
Axiall 8490 Moldings & Extrusions Flexible PVC A general purpose extrusion compound especially formulated for extruded T-moldings, tubings and other shapes where uniform flow through the die is required. Standard colors and black and natural.In.. |
|||
Specific Gravity | 1.34 - 1.40 g/cc | 1.34 - 1.40 g/cc | ASTM D 792 |
Karina 900D10/120-IS-PO White PVC Compound PVC powder compound, recommended for covering metallic parts in fluidized bed.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |