Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.32 - 1.38 g/cc | 1.32 - 1.38 g/cc | ASTM D792 |
S&E Specialty Polymers GA-1042LF PVC Application: UL bulletinized PVC based compound, suitable for injection molding application.Information provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D 792 |
Karina E800-18/258-CR-AS Gray PVC Compound UV resistant PVC compoundInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.32 - 1.38 g/cc | 1.32 - 1.38 g/cc | ASTM D 792 |
Karina SDB 35/3-LMP Ivory PVC Compound Heavy metal free PVC compound, recommended for insulation of automotive wires.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.36 - 1.38 g/cc | 1.36 - 1.38 g/cc | |
LG Chemical LK170 PVC General Description: LK170, vinyl chloride copolymer with vinyl acetate exhibit excellent properties including easy processing and effective flowMain Applications: Sealant, automotive protective sol.. |
|||
Specific Gravity | 1.32 - 1.38 g/cc @Thickness 1.57 mm |
1.32 - 1.38 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP611 Paper Base Laminate Description: Hot punching general-purpose phenolic grade. Mechanical properties approach those of NP610 with improved electrical properties and moisture resistance.Thickness Tested: 0.062", 0 125" a.. |
|||
Specific Gravity | 1.32 - 1.38 g/cc | 1.32 - 1.38 g/cc | NBR NM-IEC 60811-1-3 |
Karina 08/240-FC-LMP Beige Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.32 - 1.38 g/cc | 1.32 - 1.38 g/cc | ASTM D 792 |
Karina 42/55-GE Red Color Concentrate for PVC Heavy metal free color concentrate recommended for application in flexible and rigid PVC compounds for general purposes. Recommended use 2%.Information provided by Karina Indústria e Comércio.. |
|||
Specific Gravity | 1.32 - 1.38 g/cc | 1.32 - 1.38 g/cc | ASTM D 792 |
Karina E 20/15-RG-GE Cream Color Concentrate for PVC Color concentrate recommended for application in rigid PVC compounds for general purposes. Important Considerations:Heavy metal freeFormulated with organic and inorganic pigments PVC resin based (ca.. |
|||
Specific Gravity | 1.25 - 1.38 g/cc | 1.25 - 1.38 g/cc | ASTM D 792 |
Karina 601-48/1-BY-IS-BZ Black PVC Compound Heavy metal free, weather resistant PVC compound recommended for injection and extrusion of automotive profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.33 - 1.38 g/cc | 1.33 - 1.38 g/cc | ASTM D792 |
Spartech Royalite R86 PVC Acrylic Weather Resistant Sheet Description: Weather Resistant SheetInformation provided by Spartech. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 8510 Moldings & Extrusions Flexible PVC A general purpose, semi-rigid T-molding and extrusion compound recommended for applications where a low gloss, matte finish is desired. The compound exhibits excellent abrasion resistance.Informati.. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 8640 Moldings & Extrusions Flexible PVC General purpose extrusion compound for weatherstrips and tubings.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.32 - 1.38 g/cc | 1.32 - 1.38 g/cc | ASTM D-792 |
Axiall MP-6585 Rigid PVC, Molding Georgia Gulf MP-6585 is an electrical grade rigid vinyl injection molding compound processing good strength, stiffness, toughness, and flow. In addition, it has excellent processing stability and s.. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 13872 Wire & Cable Flexible PVC Non-lead stabilized, 720 hour sunlight resistant insulation compound recommended for TW and 75°C Class 43 applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in .. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 14771 Wire & Cable Flexible PVC General purpose jacketing compound with good low temperature properties. Recommended for a maximum service temperature of 75°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Corpor.. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 19940 Wire & Cable Flexible PVC 105°C rated insulation compound for 600V, 1/64 wall (18 AWG and larger) and 1000V applications. Approved by UL for THWN-2 (8 AWG and larger) and THW-2 in all sizes and colors. UL approved for 94 .. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 22560 Coax & Telecom Flexible PVC Semi-rigid thinwall insulation. 6+ mils.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 22880 Coax & Telecom Flexible PVC Flame retardant riser jacket over PVC or FR HDPE primaries.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 34551 Wire & Cable Flexible PVC TW, THW insulation also suitable for 105°C AWM, flex cords and Class 12/12B insulations.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 35061 Coax & Telecom Flexible PVC CMR jacket over PVC or flame retardant PE insulation with excellent low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 36631 Coax & Telecom Flexible PVC Semi-rigid, 80°C rated riser insulation compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 8808 Moldings & Extrusions Flexible PVC 105°C rated flexible polyvinyl chloride compound formulated for UL94 V-2 in all colors. The compound is formulated for sunlight resistance.Information provided by Georgia GulfGeorgia Gulf became A.. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 8906 Moldings & Extrusions Flexible PVC General purpose extrusion compound recommended for applications requiring microbial resistance and good toughness.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 12780 Coax & Telecom Flexible PVC General purpose coax cable jacket with good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 18853 Wire & Cable Flexible PVC Non-lead stabilized 105°C rated jacket suitable for FT-4 applications over PVC.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 34311 Coax & Telecom Flexible PVC CMR riser jacket over PVC or flame retardant PE insulation. Recommended for 75C applications. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorg.. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 34431 Wire & Cable Flexible PVC TW insulation. UL recognized for TW, Oil resistant I and VW-1.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.32 - 1.38 g/cc | 1.32 - 1.38 g/cc | ASTM D 792 |
Karina 06/706-RG-GE (CS) Blue Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.32 - 1.38 g/cc | 1.32 - 1.38 g/cc | ASTM D 792 |
Karina 802D18/441-CY-IS-AS-BZ Gray PVC Compound Heavy metal free PVC and weather resistant PVC compound, recommended for extrusion and injection of automotive profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 4900 Flexible PVC Non-lead stabilized, fungus resistant, 105C rated automotive insulation designed to meet the performance criteria of SAE J1128.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporat.. |