Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.02 - 1.04 g/cc | 1.02 - 1.04 g/cc | |
Michelman® Michem® Coat 50 AFN Fluorocarbon free, water and grease resistant coating Description: Fluorocarbon free, water and grease resistant coatingUsage: Michem® Coat 50AFN is an oil and grease resistant coating which also imparts good water resistance. This product is flexo .. |
|||
Specific Gravity | 1.02 - 1.04 g/cc | 1.02 - 1.04 g/cc | |
Michelman® Plate Kote™ 42S KOSHER Water based OPV Description: Water based OPV for paper platesUsage: Plate Kote™ 42S is a food-contact compliant release coating which has been formulated solely for the unique requirements of paper plate conve.. |
|||
Specific Gravity | 1.02 - 1.04 g/cc | 1.02 - 1.04 g/cc | |
Michelman® Plate Kote™ 980 KOSHER Water based OPV Description: Water based OPV for paper platesUsage: Plate Kote™ 980 is a food-contact compliant release coating which has been formulated solely for the unique requirements of paper plate conve.. |
|||
Specific Gravity | 1.02 - 1.04 g/cc | 1.02 - 1.04 g/cc | |
Michelman® Plate Kote™ 982 KOSHER Water based OPV Description: Water based OPV for paper platesUsage: Plate Kote™ 982 is a food-contact compliant release coating which has been formulated solely for the unique requirements of paper plate conve.. |
|||
Specific Gravity | 1.02 - 1.04 g/cc | 1.02 - 1.04 g/cc | |
Michelman® ThermaGloss® 460 Low odor preprint coating Description: Low odor preprint coatingUsage: ThermaGloss® 460 is a low odor preprint coating used for applications where printed / varnished liner must withstand the heat of corrugation process.T.. |
|||
Specific Gravity | 1.02 - 1.04 g/cc | 1.02 - 1.04 g/cc | |
Michelman® SofTak® 126 Non-skid coating Description: Non-skid coating.Usage: SofTak® 126 is a gluable nonskid coating with the added benefit of good scuff and water resistance, oil resistance and a "leather like" feel. This product is .. |