Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.910 - 0.950 g/cc | 0.910 - 0.950 g/cc | ASTM D792 |
S&E Specialty Polymers GPP1005HF Series PP Application: UL94 V-2, Flame-retardant polypropylene compounds for injection molding applications.Information provided by S&E Specialty Polymers |
|||
Specific Gravity | 0.910 - 0.950 g/cc | 0.910 - 0.950 g/cc | ASTM D792 |
S&E Specialty Polymers GPP1005M-EX8 PP Application: Polypropylene compound designed with halogen-based flame retardant technology meeting the UL 94 V-2 rating. Available in a wide range of colors and not subject to additive bloom.Info.. |
|||
Specific Gravity | 0.910 - 0.950 g/cc | 0.910 - 0.950 g/cc | ASTM D792-91 |
S&E Specialty Polymers GPP™ 1005M-EX10 Natural PP Application: UL94 V-2, Non-blooming flame-retardant polypropylene compound for injection moldingInformation provided by S&E Specialty Polymers |
|||
Specific Gravity | 0.910 - 0.950 g/cc | 0.910 - 0.950 g/cc | ASTM D792 |
S&E Specialty Polymers TufGuard M™ GPP1005M-CD PP, Flame Retardant Application: A UL94 V-2, flame retardant polypropylene compound for injection molding applications, including cases for industrial power supply. Compound is designed with halogen-based flame retarda.. |
|||
Specific Gravity | 0.850 - 0.950 g/cc | 0.850 - 0.950 g/cc | |
COR12V Cork/Neoprene Rubber Sheet Description: Harvested every 9-12 years from the cork oak tree, cork is able to rebound from compression with extrusion. Applications include: stoppers, soundproofing, flooring, gaskets, and many ot.. |
|||
Specific Gravity | 0.930 - 0.950 g/cc | 0.930 - 0.950 g/cc | |
Michelman® HydraBan® 708 Water resistant paper coating Description: Repulpable water resistant paper coatingUsage: HydraBan® 708 is an economical, water based treatment for kraft paper. It imparts a high degree of water repellency, is printable and g.. |
|||
Specific Gravity | 0.930 - 0.950 g/cc | 0.930 - 0.950 g/cc | |
Michelman® Michem® Wax 410 Polyethylene Description: PolyethyleneUsage: Michem® Wax 410 as an additive provides excellent block and mar resistance properties and may be used as a detackifier for synthetic and natural rubber. Food Conta.. |
|||
Specific Gravity | 0.930 - 0.950 g/cc | 0.930 - 0.950 g/cc | |
Michelman® Michem® Wood Coating 75 Anionic paraffin blend emulsion Description: Anionic paraffin blend emulsionUsage: Michem® Wood Coating 75 provides excellent water resistance for topical wood coatings. This product works to prevent the swelling of wood in the.. |
|||
Specific Gravity | 0.850 - 0.950 g/cc | 0.850 - 0.950 g/cc | ASTM D792 |
Loxim 800 00 HB Polypropylene Compound, Flame Retardant Information provided by Loxim Industries |
|||
Specific Gravity | 0.930 - 0.950 g/cc | 0.930 - 0.950 g/cc | BAM 1014 |
Kraton® G7723 G Linear Triblock Copolymer Description: Kraton G7723 GS-N is a linear triblock copolymer based on styrene and ethylene/butylene. It is supplied from North America in the physical form identified: G4610 HU - supplied as an und.. |
|||
Specific Gravity | 0.930 - 0.950 g/cc | 0.930 - 0.950 g/cc | |
Michelman® Michem® Emulsion 70750 Cationic paraffin emulsion Description: Cationic paraffin emulsionUsage: Michem® Emulsion 70350 is designed to be a water repellent additive. This product is effectively used for the curing and protection of concrete.We se.. |
|||
Specific Gravity | 0.910 - 0.950 g/cc | 0.910 - 0.950 g/cc | |
Westlake Epolene® N-10 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Product Description: Epolene N-10 is a polyethylene (PE) homopolymer that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss.. |
|||
Specific Gravity | 0.910 - 0.950 g/cc | 0.910 - 0.950 g/cc | |
Westlake Epolene® N-11P Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Information provided by Westlake Chemical |
|||
Specific Gravity | 0.910 - 0.950 g/cc | 0.910 - 0.950 g/cc | |
Westlake Epolene® N-14 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Product Description: Epolene N-14 is a polyethylene (PE) homopolymer that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss.. |
|||
Specific Gravity | 0.910 - 0.950 g/cc | 0.910 - 0.950 g/cc | |
Westlake Epolene® N-14P Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Description: Epolene N-14P is a polyethylene (PE) homopolymer powder that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss.. |
|||
Specific Gravity | 0.910 - 0.950 g/cc | 0.910 - 0.950 g/cc | |
Westlake Epolene® N-21 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Product Description: Epolene N-21 is a medium density polyethylene that improves slump resistance in cable filling and flooding, provides lubricity in printing inks, and can be used as a viscosity m.. |
|||
Specific Gravity | 0.910 - 0.950 g/cc | 0.910 - 0.950 g/cc | |
Westlake Epolene® N-21P Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Description: Epolene N-21P is a medium density polyethylene that improves slump resistance in cable filling and flooding, provides lubricity in printing inks, and can be used as a viscosity modifier.. |
|||
Specific Gravity | 0.910 - 0.950 g/cc | 0.910 - 0.950 g/cc | |
Westlake Epolene® N-30 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Product Description: Epolene N-30 is a polyethylene (PE) homopolymer that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss.. |
|||
Specific Gravity | 0.910 - 0.950 g/cc | 0.910 - 0.950 g/cc | |
Westlake Epolene® N-34 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Product Description: Epolene N-34 is a polyethylene (PE) homopolymer that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss.. |
|||
Specific Gravity | 0.910 - 0.950 g/cc | 0.910 - 0.950 g/cc | |
Westlake Epolene® N-34P Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Description: Epolene N-34P is a polyethylene (PE) homopolymer powder that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss.. |
|||
Specific Gravity | 0.910 - 0.950 g/cc | 0.910 - 0.950 g/cc | |
Westlake Epolene® N-35 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Product Description: Epolene N-35 is a polyethylene (PE) homopolymer that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss.. |
|||
Specific Gravity | 0.900 - 0.950 g/cc | 0.900 - 0.950 g/cc | ASTM D792 |
Buckeye Polymers BP FLEX 8000 VPL BLK Thermoplastic Elastomer TPV Product Information: BP Flex TPV's are partially vulcanized thermoplastic elastomers designed to meet higher end applications that require the following performance criteria.Product Features:Higher .. |
|||
Specific Gravity | 0.930 - 0.950 g/cc | 0.930 - 0.950 g/cc | ASTM D792 |
Buckeye Polymers BP FLEX D4107 CU BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Specific Gravity | 0.910 - 0.950 g/cc | 0.910 - 0.950 g/cc | |
Westlake Epolene® N-11 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Product Description: Epolene N-11 is a polyethylene (PE) homopolymer that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss.. |