Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 3.60 - 3.80 g/cc | 3.60 - 3.80 g/cc | ASTM D792 |
P & P Technology EC-H Silver Copper Loaded Fluorosilicone P & P Technology material reference EC-H is a printing grade fluorosilicone elastomer with a Silver/Copper conductive filler and is green in color. The material is specially compounded to offer exc.. |
|||
Specific Gravity | 3.60 - 4.40 g/cc | 3.60 - 4.40 g/cc | |
Parker Chomerics CHO-BOND 360-208 Conductive Epoxy Low cost, electrically conductive epoxy adhesive that combines the good adhesive characteristics as epoxy, and the superior electrical conductivity of silver. It is recommended as a thermo-setting E.. |
|||
Specific Gravity | 3.60 g/cc | 3.60 g/cc | |
Parker Chomerics CHO-BOND® 1121 General Purpose Adhesive-Sealant Silver Silicone Description: Xylene-free version of CHO-BOND 1038; rec. bond line thickness: > 0.18 mm; primer promotes adhesion CHO-BOND® 1121 is an electrically conductive, one-component silicone adhesive-sealan.. |
|||
Specific Gravity | 3.60 g/cc | 3.60 g/cc | ASTM D792 |
Parker Chomerics CHO-FORM 5526 EMI Shielding Material Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material.. |
|||
Specific Gravity | 3.60 g/cc | 3.60 g/cc | |
Resin Technology Group TIGA 905 One-Part Silver Conductive Epoxy System Cure 6 minutes at 130°C or 3 minutes at 150°C.TIGA 905 is a stress-absorbing and electrically conductive, silver-filled epoxy adhesive recommended for solder replacement in microelectronic interco.. |
|||
Specific Gravity | 3.60 g/cc | 3.60 g/cc | Mixed |
Tra-Con Tra-Duct 921U02 Long Pot Life Silver-Filled Epoxy TRA-DUCT 921U02 long room temperature pot life, silver-filled epoxy. Information provided by Tra-Con Inc. |
|||
Specific Gravity | 3.60 g/cc | 3.60 g/cc | |
Atom Adhesives AA-DUCT 904 Epoxy Adhesive AA-DUCT 904 is a single component, heat curing, conductive epoxy that was designed for ease in handling. This high performance conductive epoxy cures quickly at elevated temperatures making it ideal.. |