Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 3.30 g/cc | 3.30 g/cc | ASTM D792 |
Parker Chomerics CHO-FORM® 5518 Robotically Dispensed Gasketing Description: CHO-FORM® 5518 Two-component, thermal cure silicone system with Ag/Cu particle filler. Minimum cure temperature is only 85°C (185°F). Formulated for painted, plated or metalized plas.. |
|||
Specific Gravity | 3.30 g/cc | 3.30 g/cc | JIS-K-6220; ASTM D-792 |
Fujipoly Industries Sarcon® XR-e Gap Filler Pad Sarcon XR-e and XR-j are highly conformable/thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of compon.. |
|||
Specific Gravity | 3.30 - 3.35 g/cc | 3.30 - 3.35 g/cc | ASTM D792 |
Adamas Adalon® 826 PTFE, 50% Stainless steel Information provided by Adamas, HPM |