Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.45 - 2.95 g/cc | 2.45 - 2.95 g/cc | |
Parker Chomerics CHO-SEAL 1501 Conductive Elastomer Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics |
|||
Specific Gravity | 2.45 - 2.50 g/cc | 2.45 - 2.50 g/cc | |
Potters Industries Ballotini® Impact Beads Ballotini® impact beads are microspheres are used for precise metal finishing of parts. They offer an environmentally safe and cost effective method for metal surface cleaning and finishing. Coars.. |
|||
Specific Gravity | 2.45 g/cc | 2.45 g/cc | ASTM D792 |
Parker Chomerics THERM-A-FORM T646 Cure-in-Place Potting and Underfill Material Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co.. |
|||
Specific Gravity | 2.45 g/cc | 2.45 g/cc | |
Atom Adhesives AA-GREASE 04 Epoxy Adhesive AA-GREASE 04 is an opaque white heat sink grease compound, which is applied to the base and mounting studs of transistor and diodes to provide a positive heat sink seal, this facilitates heat transf.. |