Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.30 - 2.70 g/cc | 2.30 - 2.70 g/cc | |
Potters Industries Spheriglass® Spacer Bead Solid Soda-Lime Glass Spheres These beads are specifically designed for controlling bond line thickness in adhesive bonding. These beads are manufactured and certified to meet the specification requirements of Raytheon HMS20-177.. |
|||
Specific Gravity | 2.30 g/cc | 2.30 g/cc | |
Pyrotek NT-C Electrical Insulating Material NT-C offers superior arc and heat resistance properties, with adequate strength properties to withstand mechanical stress and hold up in severe electrical insulating applications. NT-C does not pro.. |
|||
Specific Gravity | 2.30 - 2.45 g/cc | 2.30 - 2.45 g/cc | ISO 1183 |
Raschig Group EN 5004 Epoxy Molding Compound Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo.. |
|||
Specific Gravity | 2.30 g/cc | 2.30 g/cc | JIS-K-6220; ASTM D-792 |
Fujipoly Industries Sarcon® GR-Fk Gap Filler Pad Sarcon GR-k is a general type of thermal conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and mak.. |
|||
Specific Gravity | 2.30 g/cc | 2.30 g/cc | |
GrafTech GRAFOIL® UCAR®-323 Reinforced PTFE Gasketing GRAFOIL® Grade UCAR®-323 is a laminated gasket material consisting of multiple plies of woven fiberglass coated with PTFE. It will not support combustion or bacteria. Its applications include:.. |
|||
Specific Gravity | 2.30 - 2.40 g/cc @Temperature 25.0 °C |
2.30 - 2.40 g/cc @Temperature 77.0 °F |
|
Lord Adhesives Circalokâ„¢ 6037 Epoxy Adhesive Circalokâ„¢ 6037 is an epoxy adhesive formulated for use by the semiconductor industry. An easy-to-spread thixotropic paste, it offers high heat transfer, low shrinkage, and a coefficient of ther.. |
|||
Specific Gravity | 2.30 g/cc | 2.30 g/cc | Mixed |
Tra-Con Tra-Bond 2159 Heat Conductive Electrically Insulating Compound TRA-BOND 2159 is a flexible, thermal conductive epoxy system. It is used for staking transistors, diodes, resistors, integrated circuits and other heat-sensitive components to printed circuit boards.. |
|||
Specific Gravity | 2.30 g/cc | 2.30 g/cc | Mixed |
Tra-Con Tra-Bond 2156 Heat Conductive Electrically Insulating Compound TRA-BOND 2156 is a thixotropic (smooth paste) thermally conductive epoxy system. It is used for staking heat sinks, transistors, diodes, resistor, integrated circuits and other heat-sensitive compon.. |
|||
Specific Gravity | 2.30 g/cc | 2.30 g/cc | Mixed |
Tra-Con Tra-Bond 2158 Heat Conductive Electrically Insulating Compound TRA-BOND 2158 is a flexible, thermal conductive epoxy system. It is used for staking transistors, diodes, resistors, integrated circuits and other heat-sensitive components to printed circuit boards.. |
|||
Specific Gravity | 2.30 g/cc | 2.30 g/cc | ASTM D792 |
Ecomass® 4703ZC57 Stainless Steel Filled Polyurethane Nontoxic alternative to Lead (Pb), weighting and balancing applicationsModerate Specific GravityStainless Steel Filled Polyurethane (TPU)FlexibleInformation provided by Technical Polymers |
|||
Specific Gravity | 2.30 g/cc | 2.30 g/cc | |
World Minerals Celite® Super Floss® MX Diatomaceous Earth Antiblock Additive Used as an antiblocking additive for polyethylene films. Exhibits minimal interactions with other additives in most LDPE and LLDPE resin systems.Antiblocking is accomplished via the varied particle.. |
|||
Specific Gravity | 2.30 g/cc | 2.30 g/cc | |
Aremco Pyro-Paint™ 634-SIC High Temperature Refractory Coating This advanced silicon carbide, water-based coating reduces significantly the oxidation of graphite and carbon components and structures at temperatures to 2550 °F (1400 °C). Provides a hard surfac.. |
|||
Specific Gravity | 2.30 g/cc | 2.30 g/cc | |
World Minerals Celite® Super Floss® A Diatomaceous Earth Antiblock Additive Used as an antiblocking additive for polyethylene films. Exhibits minimal interactions with other additives in most LDPE and LLDPE resin systems.Antiblocking is accomplished via the varied particle.. |
|||
Specific Gravity | 2.30 g/cc | 2.30 g/cc | |
World Minerals Celite® Super Floss® Diatomaceous Earth Antiblock Additive Used as an antiblocking additive for polyethylene films. Exhibits minimal interactions with other additives in most LDPE and LLDPE resin systems.Antiblocking is accomplished via the varied particle.. |
|||
Specific Gravity | 2.30 g/cc | 2.30 g/cc | |
World Minerals Celite® Super Floss® E Diatomaceous Earth Antiblock Additive Used as an antiblocking additive for polyethylene films. Exhibits minimal interactions with other additives in most LDPE and LLDPE resin systems.Antiblocking is accomplished via the varied particle.. |
|||
Specific Gravity | 2.30 - 3.00 g/cc | 2.30 - 3.00 g/cc | |
Reade Advanced Materials Montmorillonite - Smectite ((Na,Ca)(Al,Mg)6(Si4O10)3(OH)6-nH2O) Description: A clay mineral having a 2:1 expanding crystal lattice. Isomorphous substitution gives the various types and causes a net permanent charge balanced by cations in such a manner that water.. |
|||
Specific Gravity | 2.30 g/cc | 2.30 g/cc | ASTM D792 |
Quadrant EPP Semitron® ESd 500 HR PTFE, static dissipative, compression molded (ASTM Product Data Sheet) |