Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.23 g/cc | 2.23 g/cc | ASTM D792A |
Park Electrochemical Nelco® NX9270 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Specific Gravity | 2.23 g/cc | 2.23 g/cc | ASTM D792A |
Park Electrochemical Nelco® NX9294 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Specific Gravity | 2.23 g/cc | 2.23 g/cc | ASTM D792A |
Park Electrochemical Nelco® NX9300 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Specific Gravity | 2.23 g/cc | 2.23 g/cc | ASTM D792A |
Park Electrochemical Nelco® NX9320 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Specific Gravity | 2.23 g/cc | 2.23 g/cc | ASTM D792A |
Park Electrochemical Nelco® NY9208 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Specific Gravity | 2.23 g/cc | 2.23 g/cc | ASTM D792A |
Park Electrochemical Nelco® NY9217 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Specific Gravity | 2.23 g/cc | 2.23 g/cc | ASTM D792A |
Park Electrochemical Nelco® NY9220 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Specific Gravity | 2.23 g/cc | 2.23 g/cc | ASTM D792A |
Park Electrochemical Nelco® NY9233 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Specific Gravity | 2.23 - 2.99 g/cc | 2.23 - 2.99 g/cc | |
Parker Chomerics Tecknit Teckfip™ HC FIP-C Formed in Place Conductive Elastomer Description: Heat cure compound. This compound is an all round high performance compound, and is very similar to a Consil C molded or extruded elastomer. It has been traditionally used for telecommu.. |
|||
Specific Gravity | 2.23 g/cc | 2.23 g/cc | ASTM D4745 |
3M Dyneon™ CC607 Custom Fluoropolymer Compound
(discontinued **) This compound consists of a mixture of 35% fiberglass blended with PTFE.Information provided by Dyneon, A 3M Company |
|||
Specific Gravity | 2.23 - 2.26 g/cc | 2.23 - 2.26 g/cc | ASTM D792 |
Isoflon PTFE + 25% Glass Polytetrafluoroethylene with 25% Glass Properties:Improved compression and wear resistanceExcellent chemical stabilityBetter thermal conductivityApplications: Dynamic seals with rotating or alternating motion.Information provided by Iso.. |
|||
Specific Gravity | 2.23 - 2.25 g/cc | 2.23 - 2.25 g/cc | ASTM D792 |
Adamas Adalon® 237 PTFE, 25% Glass Fiber Information provided by Adamas, HPM |
|||
Specific Gravity | 2.23 g/cc | 2.23 g/cc | |
Asahi Glass Fluon® PA1025Z 25% Glass Fiber, PTFE Filled Compound Fluon®PTFE FC has improved creep and wear resistance. A wide range of fillers such as glass fiber, graphite, bronze, carbon fiber are available. Information provided by Asahi Glass Company, Inc. |