Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.62 g/cc | 1.62 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Rigid Extrusion L6607 Polyvinyl Chloride, Rigid (PVC, Rigid) Physical properties based on Geon L6607 white 1363Information provided by PolyOne |
|||
Specific Gravity | 1.62 g/cc | 1.62 g/cc | ASTM D792 |
Nylene® 5143 MS , 43% Glass Reinforced Low Wear Nylon 6/6 Description: Nylene® 5143 MS is a 43% glass fiber reinforced, low wear nylon 6/6. MoS2 - 2%. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies .. |
|||
Specific Gravity | 1.62 g/cc | 1.62 g/cc | ASTM D792 |
Quadrant EPP Semitron® MP-370 (ASTM Product Data Sheet) |
|||
Specific Gravity | 1.62 g/cc | 1.62 g/cc | ASTM D792 |
Polymer Resources TP-FRG30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, 30% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Specific Gravity | 1.62 g/cc | 1.62 g/cc | ASTM D792 |
Polymer Resources TPSF-FRG30 Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced, Flame RetardantProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, .. |
|||
Specific Gravity | 1.62 g/cc | 1.62 g/cc | ASTM D792 |
PolyOne Geon™ 81530 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Specific Gravity | 1.62 g/cc | 1.62 g/cc | ASTM D792 |
Gharda Chemicals Gafone™ 3610GM20 Polyethersulfone (PES)
(discontinued **) Characteristics: Excellent Thermal Resistance - Tg 224°C Outstanding Mechanical, Electrical, Flame & Chemical Resistance Very good Hydrolytic & Sterilization Resistance Good Optical Cl.. |
|||
Specific Gravity | 1.62 g/cc | 1.62 g/cc | ASTM D792 |
PolyOne Edgetek® AT-30GF/000 FDA Acetal-Copolymer, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedFDA CapablePolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Specific Gravity | 1.62 g/cc | 1.62 g/cc | ISO 1183 |
Gromax BFG50-BN00N1 Nylon 6 60% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Specific Gravity | 1.62 g/cc | 1.62 g/cc | |
Kuraray Genestarâ„¢ GN2332 Nylon, 33% Glass Filled High Flow V-0 Grade. Improves flow-ability in thin-walled parts. Used for components requiring high-flowability, such as 0.3 mm pitch connectors. |
|||
Specific Gravity | 1.62 g/cc | 1.62 g/cc | ISO 1183 |
Lanxess Pocan® BF 4130 XF 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant, improved flowabilityInformation provided by LANXESS. |
|||
Specific Gravity | 1.62 g/cc | 1.62 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1301-7767 PPS, linear, with carbon fiber, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Suitable fo.. |
|||
Specific Gravity | 1.62 g/cc | 1.62 g/cc | ISO 1183 |
Gromax BBG30-AN00N1 Nylon 6, Flame Retardant (Dry) Information provided by Gromax Enterprises Corp. |
|||
Specific Gravity | 1.62 g/cc | 1.62 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP RFL159 PA 66 LNP* LUBRICOMP* RFL159 is a compound based on Nylon 66 resin containing 25% Glass Fiber, 5% PTFE. Added features of this material include: Wear Resistant, Flame Retardant |
|||
Specific Gravity | 1.62 g/cc | 1.62 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® VB-5300GS PBT, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.62 g/cc | 1.62 g/cc | ASTM D792 |
Techmer ES Plaslube® J-80/20/TF/15 BK223 Acetal (POM) Copolymer |
|||
Specific Gravity | 1.62 g/cc | 1.62 g/cc | ASTM D792 |
Shinkong Synthetic Fibers Shinite® D202G30 PBT, 30% Glass Filled, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Specific Gravity | 1.62 g/cc | 1.62 g/cc | ASTM D 792 |
SABIC Innovative Plastics Noryl GTX APS8740 PPE+PPS (Asia Pacific) Noryl* APS8740 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can be e.. |
|||
Specific Gravity | 1.62 g/cc | 1.62 g/cc | ASTM D 792 |
SABIC Innovative Plastics Noryl GTX APS8740 PPE+PPS (Europe-Africa-Middle East) Noryl* APS8740 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can be e.. |
|||
Specific Gravity | 1.62 g/cc | 1.62 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Yellow 2600V Concentrate Based In Polyethylene DescriptionPOLYBATCH® 2600V is a yellow color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 2600V cont.. |
|||
Specific Gravity | 1.62 g/cc | 1.62 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Yellow 2600V Concentrate Based In Polyethylene DescriptionPOLYBATCH® 2600V is a yellow color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 2600V cont.. |
|||
Specific Gravity | 1.62 g/cc | 1.62 g/cc | ASTM D792 |
E-Polymers TEKASTER® F10G30FR 30% Glass Fiber Reinforced Flame Retardant PBT Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical pe.. |
|||
Specific Gravity | 1.62 g/cc | 1.62 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® VB-5300GS PBT, Glass Filled FR Information provided by Samsung Cheil Industries. |