Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.60 - 1.70 g/cc | 1.60 - 1.70 g/cc | ISO 1183 |
Raschig Group AMPLA® 2500 melamine-modified polyester Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Excellent elasticity and shock resistance, low post-shrinkage, very good electrical values, high heat.. |
|||
Specific Gravity | 1.60 - 1.75 g/cc | 1.60 - 1.75 g/cc | ISO 1183 |
Raschig Group DECAL® 1760 Phenolic Glass-fiber reinforced phenolic molding compound. Very good electrical properties, good chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals an.. |
|||
Specific Gravity | 1.60 - 1.70 g/cc | 1.60 - 1.70 g/cc | ISO 1183 |
Raschig Group MELOPLAS® 183 MF Cellulose-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in white and colored shades. Improved dimensional stability and electrical properties as compared with MP 18.. |
|||
Specific Gravity | 1.60 - 1.75 g/cc | 1.60 - 1.75 g/cc | ISO 1183 |
Raschig Group MELOPLAS® 2500 MF Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al.. |
|||
Specific Gravity | 1.60 - 1.70 g/cc @Thickness 1.57 mm |
1.60 - 1.70 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP545 Carbon Fiber
(discontinued **) Description: NP545 is composed of carbon fiber fabric and an epoxy resin system. It has excellent moisture resistance and physical properties. Potential uses include fixtures and gage systems, high .. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
Quadrant EPP Duratron® PAI T5030 Polyamide-imide, glass reinforced, extruded (ASTM Product Data Sheet) |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
LG Chemical Lupox® LW-5402 Low Warpage PBT, 40%Glass Filled, High Impact LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ISO 1183 |
Gromax BFG45-DN00N1 Nylon 6 46% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ISO 1183 |
Gromax BFM40-DL04N1 Nylon 6 40% Mineral Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ISO 1183 |
Lanxess Durethan® BKV 25 F30 000000 Nylon 6, Glass Fiber Reinforced, Flame Retardant PA 6, 25% glass fibers, injection molding, flame retardantInformation provided by LANXESS. |
|||
Specific Gravity | 1.60 - 1.66 g/cc | 1.60 - 1.66 g/cc | ASTM D 792 |
Karina E 18/601-IE MBU Gray Color Concentrate Gray pigment concentrate recommended for polyolefin, polyolefinic compound, and general PVC compound. Usage 1% minimum. Organic and inorganic.Information provided by Karina Indústria e Comérci.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
Haysite HTF Polyester, High Temp Flex HTF exhibits excellent flexibility and retention of electrical properties at elevated temperatures. For use in 220º C insulation systems in dry type transformers and where flexibility and high te.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® TK-2046H PCT, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP VERTON EV008 PEI LNP* VERTON* EV008 is a compound based on Polyetherimide containing 40% Long Glass Fiber. Added feature of this grade is: Structural. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D-792 |
Saint-Gobain Norton® Fluorglas® Chemfilm® R128/R129 Premium Grade Extruded Full Density PTFE Film (0.004" thick) Description: Full Density Unsintered Tape is used as primary insulation for high-temperature wires, jackets and cables and wall for convoluted hose. It meets the requirements of component insulation.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
A. Schulman POLYFLAM™ RCP 500 C DescriptionPolyflam® RCP 500C is an economical flame-retardant concentrate based in low-density polyethylene that features excellent dispersion and processing stability up to 550°F. ApplicationRC.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
A. Schulman POLYFLAM™ RCP 770C/CW DescriptionPolyflam® RCP 770C/CW is a flame-retardant concentrate based in low-density polyethylene that features excellent dispersion and processing stability up to 550°F.ApplicationRCP 770 C/CW.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
A. Schulman POLYFLAM™ RCP 505C Flame Retardant Concentrate Based In Low-Density Polyethylene Information provided by A. Schulman. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
Cheng Yu Plastic T885GV3 Flame Retardant PBT, 30% Glass Fiber |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
Adell WL-38 40% Glass and Mineral Reinforced PET |