Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ASTM D792 |
Ovation Polymers RIGITRON 20433 GF PBT, 33% Glass Reinforced PBT - Glass reinforced (33 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared acco.. |
|||
Specific Gravity | 1.55 - 2.05 g/cc | 1.55 - 2.05 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL 6309 Extruded Elastomer Commercial Grade Extruded Elastomer. This is an extruded nickel-plated graphite filled silicone elastomer that provides a minimum shielding effectiveness of 75 dB from 100 MHz to 10 GHz. This low co.. |
|||
Specific Gravity | 1.55 - 2.05 g/cc | 1.55 - 2.05 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL® 6510 Conductive Elastomer Extruded onlyInformation provided by Chomerics |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Flexible R1765K Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 19-7660 Polyamide 46, with glass fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Highly dimensionally stable at elevated temperatures.Gear parts for automot.. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 2205-7054 Blend based on polyaryl ether ketone, with glass fiber Applications: High dimensionally stable precision parts, high continuous use temperature.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceChemical and hydr.. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 50-8025 Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ISO 1183 |
Lanxess Pocan® ECO T 3230 000000 PBT + PET, 30% Glass Fiber PBT + PET, 30% glass fibers, injection molding, improved surface finish, contains 30% post-consumer recycled material, increased temperature peak loadInformation provided by LANXESS. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105/MS/15/TF/15 PEEK, with PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,.. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ASTM D792 |
SPS Guang Zhou PONYLâ„¢ 4002G25 Flame Retardance/GF25%-PA66 Characteristic: Good flame retardance, high mechanical properties, superior heat resistance, good dimensional stabilityApplications: E/E partsInformation Provided by SPS (Guang Zhou) Ltd. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® TK-4046H PPA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® TK-4046H PPA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP JCL36E PES LNP* LUBRICOMP* JCL36E is a compound based on Polyethersulfone (PES) resin containing 30% Carbon Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ISO 1183/1 |
A. Schulman SCHULAMID® 6 GF50H 50% Glass Fiber Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Specific Gravity | 1.55 g/cc @Temperature 25.0 °C |
1.55 g/cc @Temperature 77.0 °F |
|
Dow Corning SILASTIC® LS 4-9080 FLUOROSILICONE RUBBER Information provided by Dow Corning |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ISO 1183 |
Azoty Tarnow™ Tarnamid® T-27 GF50 Polyamide 6 - Glass Fiber Reinforced 50% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ASTM D792 |
Asahi Glass AFLAS® 100S TFE/P Fluoroelastomer AFLAS® 100/150 fluoroelastomers are alternating copolymers of tetrafluoroethylene and propylene. They offer 1) excellent heat resistance, 2) exceptional chemical resistance especially to bases and .. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ASTM D792 |
Solvay Specialty Polymers AvaSpire® AV-650 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-650 GF30 is a 30% glass fiber-reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide a high degree of chemical resistance and higher mechanical strength a.. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ASTM D792 |
PolyOne LubriOne™ PC-30GF/15T Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | ASTM D792 |
PolyOne Edgetek® RA-15GF/000 Polyethersulfone, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 V0UL 94 (CTI Testing)PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Specific Gravity | 1.55 g/cc | 1.55 g/cc | Mixed; TM R050-16 |
Resinlab® EP1240RC Flame Retardant Epoxy Casting Resin Resinlab™ EP1240RC is a medium viscosity, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File# E186034, Pro.. |