Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.47 g/cc | 1.47 g/cc | ASTM D792 |
Oxford Polymers Oxnilon 6-43GF 43% Glass Fiber Filled Nylon 6 for Injection Molding 43% Glass Fiber Filled Nylon 6 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Specific Gravity | 1.47 g/cc | 1.47 g/cc | ASTM D792 |
Quadrant EPP Acetron® MD Metal-detectable Copolymer Acetal (ASTM Product Data Sheet) Low moisture absorption High strength, stiffness Easy to machine No centerline porosity in Acetron® GP Many formulation options: Copolymer, Homopolymer, PTFE filled, and Internally lubricated/enha.. |
|||
Specific Gravity | 1.47 g/cc | 1.47 g/cc | ASTM D792 |
LNP VALOX® SMV5846 PBT + PET Alloy, 20% Carbon Fiber Reinforcement
(discontinued **) ESD ApplicationsFeatures: Good Chemical Resistance, High Flow, Flame RetardantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is .. |
|||
Specific Gravity | 1.47 - 1.53 g/cc | 1.47 - 1.53 g/cc | ASTM D 792 |
Karina 806-48/1-H-ISE-LMP Black PVC Compound Heavy metal free PVC compound.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.47 - 1.53 g/cc | 1.47 - 1.53 g/cc | NBR 14288 |
Karina 828-08/20-AY-ERYB-PO Beige PVC Compound PVC powder compound recommended for extrusion in twin screw extruder of door profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.47 - 1.53 g/cc | 1.47 - 1.53 g/cc | NBR NM-IEC 60811-1-3 |
Karina 40/14-FC-LMP Green Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.47 g/cc | 1.47 g/cc | |
Sylvin Technologies 8960-90 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Specific Gravity | 1.47 g/cc | 1.47 g/cc | +.02 |
Spartech E65695 General Purpose PVC First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B.. |
|||
Specific Gravity | 1.47 g/cc | 1.47 g/cc | |
Silberline "A" Series A-1590FG A-1590FG is an ultra fine, high opacity, non-leafing aluminum pigment for solvent based industrial coatings. Due to the small particle size, this grade is well suited for imparting high opacity at l.. |
|||
Specific Gravity | 1.47 g/cc | 1.47 g/cc | |
Silberline Sparkle Silver® 3201-ST Sparkle Silver® 3201-ST is finer in particle size than Sparkle Silver® 3141-ST, and has improved hiding properties. It is a non-leafing aluminum pigment, has brilliant sparkle, and is controll.. |
|||
Specific Gravity | 1.47 g/cc | 1.47 g/cc | ASTM D792 |
A. Schulman SCHULAMID® 66 MK4015H 40% Glass Fiber/Mineral Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Specific Gravity | 1.47 g/cc | 1.47 g/cc | ASTM D792 |
A. Schulman SCHULAMID® 66 MK4015 40% Glass Fiber/Mineral Reinforced 66 Information provided by A. Schulman. |
|||
Specific Gravity | 1.47 g/cc | 1.47 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Gold 7060E POLYBATCH® Concentrate Based In LDPE Description POLYBATCH® 7060E is a gold color concentrate based in LDPE. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 7060E is heavy meta.. |
|||
Specific Gravity | 1.47 g/cc | 1.47 g/cc | DAM; ASTM D792 |
DuPont Performance Polymers Zytel® HTN 52G35HSL NC010 Polyphthalamide (PPA) Zytel® HTN52G35HSL NC010 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds.Information provided by DuPont Performance .. |
|||
Specific Gravity | 1.47 g/cc | 1.47 g/cc | ISO 1183 |
Azoty Tarnow™ Tarnamid® T-27 GF30 TF15 Polyamide 6 - Improved Slip Properties Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Low wear and low friction grade, contains molybdenum disulfide, PTFE.Tarnamid.. |
|||
Specific Gravity | 1.47 g/cc | 1.47 g/cc | |
Aremco Ceramabind™ 542 High Temperature Inorganic Binder Single part, low viscosity, water-dispersed, aluminum phosphate solution for penetrating ultra fine thermal spray applications to 3000°F (1650°C). |
|||
Specific Gravity | 1.47 g/cc | 1.47 g/cc | ASTM D-792 |
Axiall 8150 Rigid PVC, Extrusion & Molding Georgia Gulf 8150 is a special purpose rigid PVC compound designed for applications requiring the following properties: WeatherabilityGlossImpact Strength & ToughnessFlame RetardantChemical Resista.. |
|||
Specific Gravity | 1.47 g/cc | 1.47 g/cc | ASTM D-792 |
Axiall 3240 Rigid PVC, Extrusion Georgia Gulf 3240 is a special purpose rigid powder blend PVC compound designed for applications requiring the following properties: WeatherabilityGlossImpact Strength & ToughnessFlame RetardantChe.. |
|||
Specific Gravity | 1.47 - 1.53 g/cc | 1.47 - 1.53 g/cc | ASTM D 792 |
Karina 39/47-FC-LMP Pink Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.47 g/cc | 1.47 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Gold 7060E POLYBATCH® Concentrate Based In LDPE Description POLYBATCH® 7060E is a gold color concentrate based in LDPE. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 7060E is heavy meta.. |
|||
Specific Gravity | 1.47 g/cc | 1.47 g/cc | ASTM D792 |
PolyOne LubriOne™ ATH-000/10T 2S Acetal (POM) Homopolymer
(discontinued **) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |