Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Rigid Extrusion 87180 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod te.. |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
Nylene® 9110 G43 , 43% Glass Reinforced Nylon 6/10 Description: Nylene® 9110 G43 is a 43% glass fiber reinforced specialty nylon. |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
Ovation Polymers Nemcon™ E PK DP104 Polyetheretherketone, Carbon Fiber Reinforced Nemcon™ E PK DP104 is a carbon fiber reinforced polyetheretherketone, characterized by high strength, stiffness, consistent moldabiliity, and exceptional thermal resistance.All properties after 48h.. |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining most of.. |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105-7852 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105-8417 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 19-8373 Polyamide 46, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Antistatic.Improved fri.. |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® PEKK-7299 Polyether ketone, with carbon fiber, easy flowing Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Suitable for discharging of statically generated electricity.Thermic,.. |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | |
Sylvin Technologies 8980-70 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM SF2260 PEI Blend (Asia Pacific) High flow Ultem for thin wall application |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® 815F PBT+PET (Europe-Africa-Middle East) PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | |
Shinil Chemical SHINSTRA PC/ABS SCV2030 Structural Polymer Housing SHINSTRA is the product line of structural polymer compound which exhibits excellent physical, mechanical, and thermal properties. Shinil uses the state-of-the-art dispersion and blending technolog.. |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
Techmer ES Plaslube® J-4/30/TF/13/SI/2 NAT PA6/12 |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® LH-1070W PC, FR Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP VERTON RX10409D PA 66 LNP* VERTON* RX10409D is a compound based on Nylon 66 containing proprietary fillers. Added feature of this grade is: Structural. |
|||
Specific Gravity | 1.42 g/cc @Temperature 25.0 °C |
1.42 g/cc @Temperature 77.0 °F |
|
Dow Corning SILASTIC® LS 5-8740 FLUOROSILICONE RUBBER BASE 40 Durometer off-white, molding grade fluorosilicone base.Information provided by Dow Corning |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | |
Colorite Polymers 9812-10 Radiopaque Vinyl Compound Description: Colorite radiopaque compounds are available in a variety of hardness and opacifier type. These compounds are designed for use as radiopaque striping or to be extruded into catheter tubi.. |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | |
Aremco Corr-Paint™ CP4020-S High Temperature Protective Coating Silicone-Polyester |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D-792 |
Axiall 8240 Rigid PVC, Extrusion Georgia Gulf 8240 is a general-purpose rigid PVC extrusion compound designed for applications requiring the following properties: Rigidity/StiffnessGlossImpact Strength & ToughnessFlame RetardantCh.. |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D-792 |
Axiall 5055 Rigid PVC, Extrusion, Natural Georgia Gulf 5055 is a special purpose rigid PVC compound designed for applications requiring the following properties: ToughnessUL RatingEase of ProcessingDurabilityChemical RetardantInformation p.. |