Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
Noble Polymers Ecobarrier™ 0414 Thermoplastic Olefin (TPO) Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa.. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | (Dry) |
Radici Radilon® A RV330 (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
PolyOne Geon™ Specialty Suspension CG E 24 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® CG E24 is a homopolymer specialty suspension resin intended for use in controlling gloss and transparency of injection molded, extruded or plastisol parts. This resin provides low surface glo.. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 19-7744 Polyamide 46, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert.. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
LG Chemical LUCEL FW-7005 Friction and Wear Resistant POM, Oil filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
LG Chemical Lupox® LW5102F PBT+PC+GF10% Description: Injection Molding, PBT+PC+GF10%, Low Warpage, Flame RetardantApplication: IT/OA, E&E (Switch)CAS No. 9003-01-04, 68928-70-1, 65997-17-3, 24968-12-5, 103598-77-2 and 1309-64-4Information.. |
|||
Specific Gravity | 1.40 - 1.50 g/cc @Temperature 25.0 °C |
1.40 - 1.50 g/cc @Temperature 77.0 °F |
|
Lord Adhesives Circalokâ„¢ 6031 A/B Epoxy Encapsulant Circalokâ„¢ 6031 A/B is a two-part epoxy potting compound with excellent electrical properties at elevated temperatures. Good arc-track resistance under high voltage loading and other dielectric .. |
|||
Specific Gravity | 1.40 - 1.46 g/cc | 1.40 - 1.46 g/cc | ASTM D 792 |
Karina E 805-02/196-CR Yellow PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | ISO 1183 |
Gromax BFG30-EN04B2 Nylon 6 36% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | |
Momentive Performance Materials RTV5229 Neutral Cure, One Component RTV Adhesive Sealant RTV5220 series sealants are alkoxy neutral cure, one-component, ready to use silicone adhesive sealants exhibiting low modulus/high elongation that will maintain a strong bond even when exposed to e.. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
Saint-Gobain Meldin® 5055 Thermoplastic Bearing Material General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin.. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL GFN1740V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
Shinkong Synthetic Fibers Shinite® D202 PBT, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Woodland Green 30233U/4 Concentrate Based In LLDPE DescriptionPOLYBATCH® 30233U/4 is a green color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide color and UV stability.. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Poly Off-White P90062PF Concentrate Based In Polypropylene DescriptionPOLYBATCH® P90062PF is an off-white color concentrate based in polypropylene. This concentrate was designed to provide color polypropylene film, extrusion, and molding applications. PO.. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | |
Trelleborg B570 Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
A. Schulman SCHULAMID® 66 GF33H 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
A. Schulman POLYPUR™ FPU 1515 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Specific Gravity | 1.40 g/cc @Temperature 25.0 °C |
1.40 g/cc @Temperature 77.0 °F |
|
Dow Corning 730 SOLVENT RESISTANT SEALANT Fluorosilicone (solvent resistant) RTV sealantInformation provided by Dow Corning |
|||
Specific Gravity | 1.40 - 1.415 g/cc | 1.40 - 1.415 g/cc | ASTM D792 |
Adamas Rixon 430 PEEK, 30% Carbon Fiber Information provided by Adamas, HPM |
|||
Specific Gravity | 1.40 - 1.44 g/cc | 1.40 - 1.44 g/cc | ASTM D-792 |
Axiall 375 Wire & Cable Flexible PVC General purpose and AWM flame retardant jacket. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.40 - 1.44 g/cc | 1.40 - 1.44 g/cc | ASTM D-792 |
Axiall 9148 Wire & Cable Flexible PVC Tray cable jacket. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D-792 |
Axiall 6509 Rigid PVC, Molding Georgia Gulf 6509 is a non-regulated, high flow, injection molding compound that has been specifically designed for outdoor applications that require an added degree of static resistance.Information.. |
|||
Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL FE1740PW PPE+PS (Europe-Africa-Middle East) Noryl* FE1740PW Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |