Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
PolyOne Nymax™ GF 604 35 HS Black 13 Polyamide 6 (Nylon 6) The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en.. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
S&E Specialty Polymers TufTech™ GA-3099LF PVC Compound Application: RoHS compliant, 80°C AWM insulation and jacketing compoundInformation provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
LNP ULTEM® UC3000 Polyetherimide, 30% Carbon Fiber Reinforcement
(discontinued **) High modulus with shielding/ conductive characteristics for high-heat applications.Features: Electrically Conductive, High Heat Resistance, High StrengthForms: PelletsProcessing Method: Injection Mo.. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
Ravago Manufacturing Americas Hylon® N1035HHR Nylon 66, 35% Glass Filled
(discontinued **) Heat Stabilized, Hydrolysis Resistant in Automotive CoolantInformation provided by Ravago. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
Kolon KOCETAL® LF301 Wear Modified Acetal Resin Special polymer added, improved wear property. Applications: Products for low noise and precision gear. Information provided by API-Kolon. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
LTL Color Compounds ColorFast® FRPBT200 PBT, Flame Retarded V-0 rated, unfilled PBTAll information provided by LTL Color Compounders, Inc. |
|||
Specific Gravity | 1.39 - 1.45 g/cc | 1.39 - 1.45 g/cc | ASTM D 792 |
Karina E 811-10/184-Y-CR White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
MRC Polymers EMAREXâ„¢ 400 GF33 Nylon 6/6, 33% Glass Fiber Filled Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | |
Sylvin Technologies 9980-65 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® VX5022 PBT (Europe-Africa-Middle East) VALOX VX5022 is a 20% glass fibre reinforced PBT+PC blend with low warpage characteristics. This grade is 5021 with reduced warpage. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP EC006PXQ PEI LNP* THERMOCOMP* EC006PXQ is a compound based on Polyetherimide containing 30% Carbon FIber. Added features include: Electrically Conductive, Easy Molding. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
Teknor Apex APEX® 124 Polyvinyl Chloride, Flexible Notes: 80°C Jacket; RoHS Compliant Features: Good UV Resistance; Sunlight Resistant (720 hours) Uses: Flexible Cord Jacketing; Irrigation Cable Jacketing; Military Cable Jacketing; Wire and Cable.. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
Chase Plastics CP Pryme® N333GL (COND, 50% RH) Nylon 6 (Utility Grade), 33% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Navajo 10275U/4 Concentrate Based In LDPE DescriptionPOLYBATCH® 10275U/4 is a navajo color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide color and UV stabili.. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Navajo 10275U/4 Concentrate Based In LDPE DescriptionPOLYBATCH® 10275U/4 is a navajo color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide color and UV stabili.. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Navajo 10275U/4 Concentrate Based In LDPE DescriptionPOLYBATCH® 10275U/4 is a navajo color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide color and UV stabili.. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
Colorite Polymers CS9039UL Wire and Cable Insulation Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D-792 |
Axiall NR-5009 Rigid PVC, Molding Georgia Gulf NR-5009 is an economical high flow rigid PVC fittings compound designed for multi-cavity molds and large diameter fittings. This compound is characterized by excellent processability, .. |
|||
Specific Gravity | 1.39 - 1.43 g/cc | 1.39 - 1.43 g/cc | ASTM D-792 |
Axiall 13820 Wire & Cable Flexible PVC Non-lead stabilized, 720 hour sunlight resistant insulation compound recommended for TW and 75C Class 43 applications. Good low temperature performance. Also suitable for outdoor jacket applicatio.. |
|||
Specific Gravity | 1.39 - 1.43 g/cc | 1.39 - 1.43 g/cc | ASTM D-792 |
Axiall 38900 Wire & Cable Flexible PVC Low cost AWM jacket for SPT, SVT, SJT applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
Chase Plastics CP Pryme® N233GL (COND, 50% RH) Nylon 6, 33% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Wire & Cable W2413 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
PolyOne Edgetek® UR-20GF/000 Thermoplastic Elastomer - TPU, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |