Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Wire & Cable 1725-xx13FRD Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Wire & Cable W1604L-xx07FRD Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Wire & Cable W3401 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Flexible XV3683 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
PolyOne Nymax™ GF 1204 33 HS Natural Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Flexible 90057 Polyvinyl Chloride, Flexible (PVC, Flexible) Automotive OEM approval(s).Information provided by PolyOne |
|||
Specific Gravity | 1.38 - 1.42 g/cc | 1.38 - 1.42 g/cc | PEPL-10-W-21 |
Pearl Engineering PEPLPET B101H Monofilament Resin Generally used in monofilament v-belts, zips and other technical applications. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
Daelim H&L Plavis N Aromatic Polyimide, Non-Filled, Direct Formed
(Unverified Data**) Information provided by Daelim H&L |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
Kolon KOCETAL® EL302 Toughened Grade Acetal Resin Flexible grade. Applications: Flexible products. Information provided by API-Kolon. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
LG Chemical LUMID GN-2251BF Flame Retardant PA Alloy Feature: Injection Molding, Flame Retardant PA AlloyApplication: E&E partsInformation provided by LG Chemical |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
LG Chemical LUMID GP2330B(W) PA66+GF33%, General Purpose Feature: Injection Molding, PA6+GF33%, General PurposeApplication: Automotive (Air Intake Manifold, Cylinder Head Cover)CAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ISO 1183 |
Gromax BFG30-B103N1 Nylon 6 33% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | DIN 53479 |
Isoflon PETP Polyethylene terephthalate Good optical propertiesHigh UV resistanceAbsorbs little moistureInformation provided by Isoflon. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
SPS Guang Zhou PONYLâ„¢ 4001G30 GF30%-PA66 Characteristic: High mechanical properties, superior heat resistance, good dimensional stabilityApplications: Power tool, chassis and E/E partsInformation Provided by SPS (Guang Zhou) Ltd. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | |
Shinil Chemical SHINCON PSU-CNT LCD Rack LCD Rack is used to transfer or bake LCD frame in the electronic assembly or LCD packaging assembly line. Current LCD Rack is made of poly ether ether ketone (PEEK) with carbon fiber (CF). Since b.. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | |
Silberline Sparkle Silver® 3666 Sparkle Silver® 3666 is a coarse, bright, regular purity, non-leafing aluminum pigment popular for solvent-based general industrial coatings. This pigment can be used with tints to produce a wide.. |
|||
Specific Gravity | 1.38 - 1.44 g/cc | 1.38 - 1.44 g/cc | ASTM D792 |
A. Schulman ComAlloy® E-14961 30% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Cedar 10310U Concentrate Based In LLDPE DescriptionPOLYBATCH® Cedar 10310U is a cedar color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide color and UV stabi.. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
Colorite Polymers CS6038SR Wire and Cable Insulation Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Specific Gravity | 1.38 - 1.42 g/cc | 1.38 - 1.42 g/cc | ASTM D-792 |
Axiall 8758 Moldings & Extrusions Flexible PVC A general purpose extrusion compound recommended for extruded shapes, weatherstrips and flexible gaskets. Formulated for good UV light resistance and low temperature properties.Information provided.. |
|||
Specific Gravity | 1.38 - 1.42 g/cc | 1.38 - 1.42 g/cc | ASTM D-792 |
Axiall 8910 Moldings & Extrusions Flexible PVC Extrusion compound especially formulated for extruded T-moldings, tubings, and other shapes where uniform flow through the die is required.Information provided by Georgia GulfGeorgia Gulf became Axi.. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | |
Trelleborg Commercial Neoprene® C803 Chloroprene CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade.. |
|||
Specific Gravity | 1.38 - 1.42 g/cc | 1.38 - 1.42 g/cc | ASTM D-792 |
Axiall 1055 Wire & Cable Flexible PVC NM-B and UF-B jacket with good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | |
Sylvin Technologies 9812A-70 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |