Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.28 g/cc | 1.28 g/cc | ASTM D792 |
RedEye On Demand Polyphenylsulfone (PPSF), Rapid Prototyping Material Polyphenylsulfone (PPSF) is a durable high-end thermoplastic that can be used in the toughest applications. Parts built in PPSF can handle heat near 400°F (204°C), it resists petroleum products, a.. |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | ASTM D792 |
SABIC Innovative Plastics Lexan® ML4249 PC Polycarbonate for aircraft applications requiring FAR 25.853a compliance. Transparent, transluscent and opaque colors. For blow molding. |
|||
Specific Gravity | 1.28 - 1.32 g/cc | 1.28 - 1.32 g/cc | ASTM D 792 |
Karina E CAK 65-48/1 Black PVC Compound Reclaimed PVC compound recommended for soles injectionInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 20/AF/15/TF/10 Polyphthalamide, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low influence from moisture an.. |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 3/CF/30/EG Polyamide 6, with carbon fiber, extrusion grade Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressElectrically conductive, suitable.. |
|||
Specific Gravity | 1.28 - 1.34 g/cc | 1.28 - 1.34 g/cc | ASTM D 792 |
Karina 842-IS-SD Crystal PVC Compound PVC compound recommended for extrusion of sheet for vacuum forming (blister).Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1-7360/EG Polyamide 66, with PTFE, lubricant modified, high viscosity, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property.Bea.. |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM CRS5011 PEI Transparent, Enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 listing. |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | ASTM D 792 |
SABIC Innovative Plastics Ultem DH1004F PEI (Asia Pacific) High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Asia Pacific .. |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | ASTM D 792 |
SABIC Innovative Plastics Ultem DT1810E PEI Blend Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Americas re.. |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM DT1810EV PEI Blend Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming, UL94 V0 listed. |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | ASTM D792 |
Spartech Royalstatâ„¢ R632 ABS/PVC Static Control Sheet Description: Static Control SheetInformation provided by Spartech. |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON Noryl_FMC3008A PPE+HIPS (Europe-Africa-Middle East) LNP* Stat-kon* Noryl_FMC3008A compound is a 30% carbon fiber/glass/mineral filled, static dissipative, foamable resin. UL94 V1 rated. Property values at 20% weight reduction, 0.250"" wall. |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC3008A PPE+HIPS (Europe-Africa-Middle East) LNP* Stat-kon* Noryl_HMC3008A compound is a 30% glass/mineral/carbon fiber reinforced resin; static dissipative; 250F (120C) HDT. Tight tolerance molding. |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_SP7602 PC (Asia Pacific) |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | 23°C; ASTM D792 |
Teknor Apex MF 141 Polyvinyl Chloride, Flexible Film Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Film, Medical Applications Forms-PelletsAppearance-ClearInformation provided by Teknor Apex Company |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | |
Struktol VM 512 LUBRICANT ADDITIVE FOR PVC AND POLYMER PROCESSING Blend of mineral additives in a polymer carrier.Applications: STRUKTOL® VM-512 is a matting agent for rigid PVC to produce a matted/textured surface. It is ideal for water channeling applications.. |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Green 3315 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 3315 is a green color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 3315 is typi.. |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | ASTM D792 |
A. Schulman SCHULAMID® 66 MK20HI 20% Mineral Reinforced, Impact Modified Nylon 66 Information provided by A. Schulman. |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Brown 10306 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 10306 is a brown color concentrate based in linear low density polyethylene. This product was formulated to offer color and opacity in polyethylene film applications. POLYBA.. |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | |
Trelleborg B569 Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Specific Gravity | 1.28 - 1.32 g/cc | 1.28 - 1.32 g/cc | ASTM D-792 |
Axiall 830B Wire & Cable Flexible PVC 80°C rated compound recommended for UL 360, liquid tight flexible conduit jacket applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | |
Aremco Corr-Paint™ CP4020 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4010 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR N330 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Specific Gravity | 1.28 g/cc | 1.28 g/cc | ASTM D792 |
GEHR Plastics ECOGEHR® C-L Cellulose-Lignin Compound
(discontinued **) C-L is comprised of the wood components cellulose, natural fibers, lignin and fatty acids. It possesses many interesting properties that together are very similar to the natural wood. Consequently,.. |