Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Packaging 4195 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
SABIC Innovative Plastics Lexan® EXL4019 PC Lexan* EXL4019 is an opaque 9% Glass Fiber (GF) reinforced polycarbonate (PC) siloxane copolymer resin for injection molding (IM) applications requiring improved stiffness. This resin also offers im.. |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer (Asia Pacific) Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele.. |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR N339 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Specific Gravity | 1.25 - 1.35 g/cc @Thickness 1.57 mm |
1.25 - 1.35 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP680 Paper Base Laminate Description: Hot punching grade with electrical properties between NP611 to NP631.Thickness Tested: 0.062", 0.125" & 0.500" |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
LG Chemical LUPOY GN2101F PC+GF10%, Halogen Free, Flame Retardant, Heat Resistance Description: Injection Molding, PC+GF10%, Halogen Free Flame Retardant, Heat ResistanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information prov.. |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | +.02 |
Spartech E65090 General Purpose PVC First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B.. |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC (Europe-Africa-Middle East) Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | 23°C; ASTM D792 |
Teknor Apex APEX® 90-A472R-85-NT Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Medical Applications, Caps, Closures, Valves/Valve Parts Appearance-ClearForms-PelletsProcessing Method-.. |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
Samyang Trirex® 3025GN10 Polycarbonate, Reinforced Flame Retardancy PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3025GN10 is a reinforced flame retardant grade.Applications: LCD Panel Frame (dimensio.. |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
Teknor Apex MF 09-G0288A-87NT Polyvinyl Chloride, Flexible Film Uses: Medical/Healthcare Applications Forms: FilmInformation Provided by Teknor Apex |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
Teknor Apex Sinvicomp SFE 5000 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Food Contact Acceptable; Non-Toxic Uses: Hose; Tubing Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
A. Schulman ComAlloy® 510-3010 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
A. Schulman COMTUF® 5011 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman. |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
A. Schulman ComAlloy® 510-3010 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FXP 1245U UV Stable Copolymer Polypropylene DescriptionPolyfort® FXP 1245U is a 40% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman. |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
Cheng Yu Plastic N6GV25 Flame Retardant Nylon 6, 25% Glass Filled |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
Clariant Renol PC010-L FR Polycarbonate, Glass Reinforced, Flame Retardant Data provided by Clariant Masterbatches |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | |
Colorite Polymers 8512 Clear Injection Molding Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c.. |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
Colorite Polymers 8566 Non-Phthalate 66 Series Vinyl Compound Description: The Colorite 66 series is a family of non-toxic PVC compounds developed specifically for those medical device, food, and infant care items for which the use of a citrate* based non-phth.. |
|||
Specific Gravity | 1.25 - 1.29 g/cc | 1.25 - 1.29 g/cc | ASTM D-792 |
Axiall EX1188A Wire & Cable Flexible PVC UL 360 jacket compound. 80°C air; 60°C oil.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.25 - 1.29 g/cc | 1.25 - 1.29 g/cc | ASTM D-792 |
Axiall 18753 Wire & Cable Flexible PVC Non-lead stabilized, fungus resistant 105 C rated jacket compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
Samyang Triel® 5720 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5720 is an extrusion grade.Information provided by Samyang. |
|||
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FXP 1245U UV Stable Copolymer Polypropylene DescriptionPolyfort® FXP 1245U is a 40% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman. |