Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
Network Polymers NPP Nylon 66G13L Description: NylonInformation provided by Network Polymers Inc. |
|||
Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
Polymer Resources PC-GP2-TFE5 Polycarbonate, 5% PTFE, Wear Resistant, Medium Flow Polycarbonate, 5% PTFE, General Purpose, Medium Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samp.. |
|||
Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
LG Chemical LUMID GP2130B(W) PA66+GF13%, General Purpose Feature: Injection Molding, PA66+GF13%, General PurposeApplication: Valve CoversCAS No. 32131-17-2, 65997-17-3 and 9010-79-9Information provided by LG Chemical |
|||
Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
LG Chemical LUPOY GP-1006F General Purpose Modified PC, Unreinforced, Weather Resistant, Flame Retardant Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Specific Gravity | 1.22 - 1.28 g/cc | 1.22 - 1.28 g/cc | ASTM D 792 |
Karina E 06/40-RG-PO Blue Color Concentrate for PVC Color concentrate in powder form recommended for application in PVC compounds for general purposes extrusion and injection. Recommended to use 2%.Information provided by Karina Indústria e ComÃ.. |
|||
Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM 792 |
Multibase Multi-Flex® A 7455 ER TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP C7410 PC+ABS (Asia Pacific) LNP* Thermocomp* C7410 compound is a talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications. |
|||
Specific Gravity | 1.22 g/cc | 1.22 g/cc | 23°C; ASTM D792 |
Teknor Apex MF 170 NT Polyvinyl Chloride, Flexible Film Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Film, Medical Applications Forms-PelletsAppearance-ClearInformation provided by Teknor Apex Company |
|||
Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-2740L3-UV Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66 Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
Lubrizol ESTANE® 5707 Ester Based Thermoplastic Polyurethane Features: Very high tensile strength, excellent low temperature flexibility and superior abrasion and cut resistance. It is processed by means of solution coating, extrusion and melt coating.Uses: S.. |
|||
Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
Lubrizol Estane® 58610 Thermoplastic Polyurethane Features: Combines flexibility, toughness and excellent roll release for calendering and melt coating applications.Uses: Injection molding and general extrusion techniques. It is used in film, shee.. |
|||
Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 3717 Talc Filled Homopolymer Polypropylene (39.6% Mineral Content) DescriptionPolyfort® FPP 3717 is a 40% talc filled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Specific Gravity | 1.22 g/cc | 1.22 g/cc | Mixed |
Tra-Con Tra-Bond 2115 Clear High Strength Epoxy Adhesive TRA-BOND 2115 is a clear, low viscosity epoxy formulation used in the fabrication of lasers. It is capable of withstanding 30 seconds of 60 watt direct laser energy. The low cure shrinkage (using a .. |
|||
Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
A. Schulman POLYBLAK™ 3123 Premium Black Color Concentrate, 50% Carbon Black Based In LDPE DescriptionPOLYBLAK® Black 3123 is a premium black color concentrate containing 50% carbon black in LDPE. This masterbatch is designed to provide good opacity and a regular blue undertone with pig.. |
|||
Specific Gravity | 1.22 g/cc | 1.22 g/cc | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Specific Gravity | 1.22 g/cc | 1.22 g/cc | Part B |
Epoxy Technology EPO-TEK® 377 High Temperature Epoxy Product Description: EPO TEK®377 is a two component, high Tg, fiber optic grade epoxy adhesive. It is well suited for semiconductor, medical and optical applications.Advantages & Application Notes:.. |
|||
Specific Gravity | 1.22 g/cc | 1.22 g/cc | Part B |
Epoxy Technology EPO-TEK® CF6-2 High Temperature Epoxy Product Description: EPO-TEK® CF6-2 is a two component, high temperature and high Tg epoxy designed for fiber optic packaging. Advantages & Application Notes: The low viscosity nature allows for wi.. |
|||
Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
Diamond Polymers NPP 808 C8 TDS Polycarbonate Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
Colorite Polymers 7500 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
Colorite Polymers 7577 Non-Phthalate 77 Series Vinyl Compound Description: The Colorite 77 series is a family of compounds designed for those medical device producers that require the use of a non-phthalate plasticizer that has superior resistance to extractio.. |
|||
Specific Gravity | 1.22 g/cc | 1.22 g/cc | @75°C |
ACC EP A 32 EPI Engineered Polymers MDI EP A 32, “Powered by Reactamine® Technology”, is a mixture of 4,4 and 2,4 MDI with a low viscosity. EP A 32 has stability at low temperatures, and is useful for making elastomers and prepolymers... |
|||
Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
Aaron Industries AAROPRENE® GFABS 4020 Glass Filled Acrylonitrile-Butadiene Styrene AAROPRENE® GFABS 4000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
Aaron Industries AAROPRENE® GFPP 2040 Glass Filled Polypropylene AAROPRENE® GFPP 2000 Series Glass Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
Teknor Apex Sinpolene CPP1040 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Calcium Carbonate Filler, 40% Filler by Weight Features: Homopolymer Uses: Appliance Components; Furniture; Housings F.. |
|||
Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
E-Polymers TEKAPPO® JF101 Filler Reinforced Heat Resistant Dimensional Stability Flame Retardant M-PPO Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a.. |