Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D792 |
Nylene® Naxel™ PC30 Polycarbonate Description: Naxel™ PC30 is a 25 melt, general purpose polycarbonate. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources .. |
|||
Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D792 |
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D792 |
SABIC Innovative Plastics Lexan® 123 PC (Asia Pacific) Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. |
|||
Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D792 |
SABIC Innovative Plastics Lexan® 221R PC (Asia Pacific) 17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. |
|||
Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D792 |
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer (Asia Pacific) 11 MFR LEXAN High Flow Ductile Copolymer |
|||
Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D792 |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC (Europe-Africa-Middle East) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D792 |
SABIC Innovative Plastics Lexan® SLX2431T PC Copolymer (Asia Pacific) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D792 |
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer (Europe-Africa-Middle East) XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Flexible XV3772 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D792 |
SABIC Innovative Plastics Lexan® 141 PC General purpose polycarbonate with melt flow rate of 10.5. |
|||
Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D792 |
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer (Asia Pacific) 11 MFR LEXAN High Flow Ductile Copolymer UV stabilized |
|||
Specific Gravity | 1.20 - 1.26 g/cc | 1.20 - 1.26 g/cc | ASTM D 792 |
Karina E KAPU 6535/1-NT-MARFIM Ivory Compound (SP31502) Kapu-Ivory microexpanded compound.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.20 g/cc | 1.20 g/cc | |
LG Chemical BPA Structure & Characteristics: (CH3)2C(C6H4OH)2 . BPA is an us powder with white colorOverview: Bisphenol-A(BPA) is used primarily to make polycarbonate and epoxy resins, both of which are used in a w.. |
|||
Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D792 |
LG Chemical Lupoy 1201-15 Polycarbonate Resin Description: LUPOY PC 1201-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D792 |
Star Plastics PC1212R Molding Grade PC with Release Information provided by Star Plastics, Inc. |
|||
Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D792 |
Styron CALIBREâ„¢ 302-06 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D792 |
Teknor Apex APEX® 3300R-75NT Polyvinyl Chloride, Flexible Notes: RoHS Compliant Uses: Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex |
|||
Specific Gravity | 1.20 g/cc | 1.20 g/cc | ISO 1183 |
Ter Hell Plastic Terez® PA 6 7751 TGF 15 GL Polyamide 6, 15% Glass Fiber Description: Medium viscosity, dry impact resistant PA 6, 15% glass fiber reinforced and improved surface gloss.Application: For molding parts with good stiffness and high dimensional stability.In.. |
|||
Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D792 |
Chase Plastics CP Pryme® PC100R Polycarbonate Molding Resin, Mold Release Information provided by Chase Plastics. |
|||
Specific Gravity | 1.20 - 1.25 g/cc | 1.20 - 1.25 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman. |
|||
Specific Gravity | 1.20 g/cc | 1.20 g/cc | Redux 870 A |
Hexcel® Redux® 870 A/B Two Component Shimming and Potting Epoxy Paste Adhesive Redux 870 A/B is a two component high performance epoxy paste adhesive, ideal for use as a Liquid Shim or for potting applications. This high temperature performing thixotropic adhesive has been spe.. |
|||
Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D792 |
E-Polymers TEKANATE® G7020 General Purpose Easy Molding Polycarbonate Modified Poly Carbonate: TEKANATE is a modified PC by improving polycarbonate resins with features of halogen-free flammability, transparency, impact resistance and reinforced fiberglass. It shows .. |
|||
Specific Gravity | 1.20 g/cc | 1.20 g/cc | catalyzed with QM CAT BLUE |
ACC QM 107 QSI Quantum Silicones 7 Durometer Condensation Cure Moldmaking Material QM 107 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is us.. |
|||
Specific Gravity | 1.20 g/cc | 1.20 g/cc | uncured |
Atom Adhesives AA-BOND 2103 Epoxy Adhesive AA-BOND 2103 is a clear, near transparent, medium viscosity epoxy adhesive formulation developed for rigid laminating, sealing and bonding applications where the combination of good wetting and impr.. |
|||
Specific Gravity | 1.20 g/cc | 1.20 g/cc | "A" component |
ACC QSil 40 QSI Quantum Silicones 40 Durometer Condensation Cure for Potting QSil 40 is a general purpose two-part, room temperature, condensation cure siloxane elastomer. The two applicable catalysts are 0.5% DBT by weight and 10% Deep Section Catalyst by weight. Cure speed.. |
|||
Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D 792 |
SABIC Innovative Plastics Lexan® EXRL0681 PC Copolymer 25 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region. |
|||
Specific Gravity | 1.20 g/cc | 1.20 g/cc | 23°C; ASTM D792 |
Teknor Apex APEX® 3302-65 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses- Medical Applications, Tubing, Appearance-ClearForms-PelletsProcessing-ExtrusionInformation provided by.. |
|||
Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D792 |
Teknor Apex Sinvicomp SFC 8000 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Foamable Uses: Footwear Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D792 |
SABIC Innovative Plastics Lexan® HFD1711 PC Copolymer (Asia Pacific) 25 MFR LEXAN High Flow Ductile Copolymer |