Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.09 g/cc | 1.09 g/cc | 23/23°C; ASTM D792 |
RheTech Products HP519-00 26% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trim moldingsSill platesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 1.09 g/cc | 1.09 g/cc | |
Resinlab® CYNERGY CA6105 Adhesive Description: The CYNERGY 6100 SERIES products are used to bond metal to itself or other substrates. It is available in five standard viscosities.Application: The CYNERGY SERIES of the cyanoacrylates.. |
|||
Specific Gravity | 1.09 g/cc | 1.09 g/cc | Part B; TM R050-16 |
Resinlab® EP1385 Black Epoxy Formulation Resinlab™ EP1385 Black is an epoxy formulation designed for applications requiring resistance to E-85 type fuels. It has good wetting and adhesion to most surfaces. It has very good resistance to w.. |
|||
Specific Gravity | 1.09 g/cc | 1.09 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 6-8436 Polyamide 12, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Dynamic stressed parts.Low waterabsorbtion.Isotropic shrinkage characteristics.Bearings, sleeve.. |
|||
Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D792 |
Fiberfil® PP-60/TC/24/D/HS Polypropylene Homopolymer, Talc Filled, Heat Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Specific Gravity | 1.09 - 1.13 g/cc | 1.09 - 1.13 g/cc | |
LG Chemical CP-WB Polycarboxylic Copolymer Description: CP-WB is the main raw material for concrete admixture, which improves water reducing and slump retention abilities. CP-WB was developed through our advanced synthetic technologies, impa.. |
|||
Specific Gravity | 1.09 g/cc | 1.09 g/cc | DBPH Cure |
Shin-Etsu Silicones SV-14000U Silicone Rubber SV14000U is one of a series of easy processing, no post cure silicone rubber bases. It can be used in a variety of applications requiring finishing by molding, extruding or calendering. Product Feat.. |
|||
Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp FF004 PE LNP THERMOCOMP* FF004 is a compound based on Polyethylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D792 |
Samsung Cheil Industries Starex® LX-0989EXS ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D 792 |
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66 (Asia Pacific) High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL WCD851 PPE-TPE (Asia Pacific) Flexible, strong flame-retardant, halogen-free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame retardant performance capable of meeting UL VW-.. |
|||
Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D792 |
Teknor Apex Telcar® TL-8712 Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou.. |
|||
Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D792 |
Teknor Apex Telcar® TL-91-T3056D-75 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D792 |
A. Schulman POLYTROPE™ TPP 620 Olefinic Elastomer DescriptionPolytrope TPP 620is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 620 is des.. |
|||
Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Silver 7002/5 Concentrate Based In LDPE DescriptionPOLYBATCH® 70022/5 is a silver color concentrate based in LLDPE. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® 70.. |
|||
Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D792 |
A. Schulman POLYTROPE™ TPP 620 Olefinic Elastomer DescriptionPolytrope TPP 620is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 620 is des.. |
|||
Specific Gravity | 1.09 g/cc @Temperature 25.0 °C |
1.09 g/cc @Temperature 77.0 °F |
|
Dow Corning LSPBK26 SILICONE MASTERBATCH BLACK Information provided by Dow Corning |
|||
Specific Gravity | 1.09 g/cc @Temperature 25.0 °C |
1.09 g/cc @Temperature 77.0 °F |
|
Dow Corning SILASTIC® T-4 RTV SILICONE RUBBER BASE & CURING AGENT Translucent, high tear strength moldmaking rubber featuring fast cure. Suited for prototype design and production tooling. Silastic T-4 is recommended for use with rigid polyurethane and can be used.. |
|||
Specific Gravity | 1.09 g/cc @Temperature 25.0 °C |
1.09 g/cc @Temperature 77.0 °F |
|
Dow Corning SILASTIC® T-4 RTV SILICONE RUBBER BASE & T-4 O CURING AGENT Translucent, oil bleeding high strength silicone mold making rubber that features high tear with fast cure. Suited for prototype design and production tooling. Silastic T-4 O is recommended for use .. |
|||
Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D792 |
Diamond Polymers ABS 4011 HH Description: Ultra High Heat ABSInformation provided by Diamond Polymers, Inc. |
|||
Specific Gravity | 1.09 g/cc | 1.09 g/cc | 23°C; ASTM D792 |
Asahi Kasei Xyron® X5402 PPE/PA Oil ResistantInformation provided by Asahi Kasei |
|||
Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D792 |
Bhansali Engineering Abstron TIM 200 MMA- ABS High Impact(Transparent ABS)Information provided by Bhansali |
|||
Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D792 |
Bhansali Engineering Abstron TIM 200 MMA- ABS High Impact(Transparent ABS)Information provided by Bhansali |
|||
Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D792-66 |
BCC Products BC 8405 Urethane Casting BC8405 is an unfilled, low viscosity, quick setting two component urethane system. When properly cured, BC 8405 will exhibit high impact strength and yield thermoplastic-like parts. Some features i.. |
|||
Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D792 |
Ravago Manufacturing Americas Echo® RPC20FG BK Polypropylene Homopolymer Available in North America Filler: Glass Fiber Reinforcement, 20% Filler by weight Recycled Content: YesFeatures: Homopolymer Color: Black Form: Pellets Information provided by Ravago |
|||
Specific Gravity | 1.09 g/cc | 1.09 g/cc | |
Resinlab® CYNERGY CA6905 Adhesive Description: The CYNERGY 6900 SERIES are for use in demanding applications where very fast cure speeds and high temperature resistance are required. These are single component solvent free materials.. |