Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.007 g/cc @Temperature 25.0 °C |
1.007 g/cc @Temperature 77.0 °F |
|
Dow Corning ES-5612 Silicone Formulation Aid Produces W/Si and W/Si+O emulsions with textures that range from lotion to cream, leaving a light, nongreasy after feel on the skin.It is a low molecular weight ethoxylated silicone surfactant.Dow C.. |