Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.980 g/cc | 0.980 g/cc | ASTM D792 |
PolyOne Maxxam™ FR PE 112 LDPE
(discontinued **) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | ASTM D792 |
Fiberfil® PP-68/V2 Polypropylene Copolymer, Flame Retardant, UL94 V2 Information provided by FIBERFIL Engineered Plastics |
|||
Specific Gravity | 0.980 - 1.02 g/cc | 0.980 - 1.02 g/cc | |
Michelman® Michem® In-Line Primer Q4305A Primer Description: Michem® In-Line Primer Q4305A is a primer for print receptivity for use with HP Indigo press W3250.Usage: Michem® In-Line Primer Q4305A is designed as a primer for HP Indigo subst.. |
|||
Specific Gravity | 0.980 - 1.00 g/cc | 0.980 - 1.00 g/cc | |
Michelman® Michem® Prime 2960 Ethylene acrylic acid dispersion Description: Ethylene acrylic acid dispersionUsage: Michem® Prime 2960 provides outstanding adhesion to both metallic and cellulosic substrates, and enhances the water, grease, oil and solvent re.. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | ASTM D792 |
Lucent Polymers CPP-110 Polypropylene Homopolymer, 10% Calcium Carbonate Filled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | ASTM D792 |
Lucent Polymers TPP-110 Polypropylene, Homopolymer, 10% Talc Filled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Specific Gravity | 0.980 - 1.00 g/cc | 0.980 - 1.00 g/cc | |
Michelman® Michem® Emulsion 93135M Nonionic polyethylene emulsion Description: Nonionic polyethylene emulsionUsage: Michem® Emulsion 93135M is a phenol and formaldehyde free wax emulsion used in floor polish formulations for black heel mark resistance, toughnes.. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON MX12407C PP LNP* STAT-KON* MX12407C is a compound based on Polypropylene resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding System. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | |
Struktol TR EBS Processing Additive, Dispersant N,N` Ethylene Bis-stearamideSTRUKTOL® TR EBS is an exceptionally effective dispersion aid for a wide range of organic and inorganic pigments. STRUKTOL® TR EBS can be used in most polymer carri.. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-1426A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ FSU-105-E Concentrate Based In LDPE DescriptionPOLYBATCH® FSU-105-E is a general purpose erucamide slip and antiblock concentrate based in LDPE. This material has been designed to offer a 2:1 antiblock slip ratio for films whose COF.. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | ASTM D792 |
A. Schulman POLYTROPE™ TPP 518 Injection Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 518 is an injection grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal expansion i.. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | |
Zeon Chemicals Nipol® 1052 Nitrile Elastomer Nipol 1052 is a copolymer of butadiene and acrylonitrile with medium oil resistance. Sufficient non-staining antioxidant is added during manufacture for normal storage conditions.Excellent general p.. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | |
Zeon Chemicals Nipol® 1052-30 Nitrile Elastomer Nipol 1052-30 is a copolymer of butadiene and acrylonitrile with medium oil resistance. Sufficient non-staining antioxidant is added during manufacture for normal storage conditions.Low Mooney versi.. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | |
Zeon Chemicals Zetpol® 1020 Hydrogenated Nitrile Elastomomer Zeptol 1020 is a highly saturated copolymer of butadiene and acrylonitrile with high tensile strength, good heat resistance, good chemical resistance to aggressive fluids, and an excellent balance o.. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | |
Zylog Hipolyene® 1048 X1 Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ FSU-105 Concentrate Based In LDPE DescriptionPOLYBATCH® FSU-105 is a general-purpose oleamide slip and antiblock concentrate based in LDPE. This material has been designed to offer a 2:1 antiblock slip ratio for films whose COF va.. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | |
Zeon Chemicals Nipol® 1072x28 Carboxylated Nitrile Elastomer Nipol® nitrile elastomers are recommended when oil or solvent resistance is needed for the proper functioning of rubber parts. Fuel, oil and solvent resistance improves as acrylonitrile content is .. |
|||
Specific Gravity | 0.980 g/cc @Temperature 25.0 °C |
0.980 g/cc @Temperature 77.0 °F |
|
Dow Corning AP-8087 FLUID This amino functional siloxane polymer can be used in a range of hair care applications including shampoos, rinse-off conditioners, leave-in conditioning treatments, colorants, and styling products... |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | 15°C; ASTM D1298 |
ExxonMobil 32 Mobil EAL Arctic Series Mobil EAL Arctic Series are high performance Environmental Awareness Lubricants (EAL) that are fully synthetic products designed specifically for the lubrication of refrigeration compressors and sys.. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | Uncatalyzed, QM 260B |
ACC QM 260 QSI Quantum Silicones 60 Durometer Addition Cure Moldmaking Material QM 260 is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is a good choice for th.. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | |
Zeon Chemicals Nipol® 33-3 Nitrile Elastomer General-purpose, low-viscosity nitrile rubber. Designed for injection modling and resistance to mold fouling.General purpose, low viscosity nitrile rubber. Designed for injection molding and resista.. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | |
Zeon Chemicals Nipol® DN3335 Nitrile Elastomer Nipol DN3335 is a copolymer of butadiene and acrylonitrile with medium oil resistance. Sufficient non-stainign antioxidant is added during manufacture for normal storage conditions.Low mold fouling,.. |
|||
Specific Gravity | 0.980 g/cc | 0.980 g/cc | |
Zeon Chemicals Nipol® DN1201 Terpolymer Elastomer Nipol DN1201 is a low-temperature polymerized terpolymer of acrylonitrile, butadiene and isoprene. This polymer is intended to give better physical and processing characteristics than a conventional.. |