Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.978 g/cc | 0.978 g/cc | ASTM D792 |
PolyOne Maxxam™ FR PP 301 S Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Specific Gravity | 0.978 - 0.984 g/cc @Temperature 25.0 °C |
0.978 - 0.984 g/cc @Temperature 77.0 °F |
ASTM D4052 |
PolyOne reFlex™ 300 Plasticizer, Bio-derived Bio-derived, non-phthalate plasticizer; USDA BioPreferred® certified 99% biobased.Information provided by PolyOne |
|||
Specific Gravity | 0.978 - 0.984 g/cc @Temperature 25.0 °C |
0.978 - 0.984 g/cc @Temperature 77.0 °F |
ASTM D4052 |
PolyOne Synplast™ DOP-N Di (2-ethylhexyl) Phthalate Branched C8 phthalate esterInformation provided by PolyOne |
|||
Specific Gravity | 0.978 - 0.984 g/cc @Temperature 25.0 °C |
0.978 - 0.984 g/cc @Temperature 77.0 °F |
ASTM D4052 |
PolyOne Synplast™ NOTM-E Tri (n-octyl) Trimellitate Linear trimellitate esterContains 0.10-0.15 wt% 1,1,3-Tris (2-methyl-4hydroxy-5-t-butyl phenyl) butane antioxidantInformation provided by PolyOne |
|||
Specific Gravity | 0.978 - 0.984 g/cc @Temperature 25.0 °C |
0.978 - 0.984 g/cc @Temperature 77.0 °F |
ASTM D4052 |
PolyOne Synplast™ NOTM-PPC Tri (n-octyl) Trimellitate CPSIA HR 4040 Compliant Linear trimellitate esterContains 0.10-0.15 wt% 1,1,3-Tris (2-methyl-4hydroxy-5-t-butyl phenyl) butane antioxidantInformation provided by PolyOne |
|||
Specific Gravity | 0.978 g/cc | 0.978 g/cc | ASTM D792 |
PolyOne Versaflex™ HC 2110-43N Thermoplastic Elastomer (TPE) Versaflex™ HC 2110-43N is a unique TPE designed for the demanding requirements of gaskets and stoppers used in healthcare and food packaging applications. New Product. Commercial specifications hav.. |
|||
Specific Gravity | 0.978 g/cc | 0.978 g/cc | ASTM D792 |
PolyOne Maxxam™ FR PP 301 Black 1284-11 S Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Specific Gravity | 0.978 g/cc | 0.978 g/cc | ASTM D792 |
PolyOne Maxxam™ FR PE 112 LDPE
(discontinued **) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Specific Gravity | 0.978 g/cc | 0.978 g/cc | ASTM D792 |
PolyOne Elastamax™ XL 0131-61 Styrene Butadiene Block Copolymer (SBC)
(discontinued **) A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in acco.. |
|||
Specific Gravity | 0.978 g/cc | 0.978 g/cc | ASTM D792 |
PolyOne Elastamax™ XL-0153-79 Styrene Butadiene Block Copolymer (SBC)
(discontinued **) A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in acco.. |
|||
Specific Gravity | 0.978 g/cc | 0.978 g/cc | |
Teknor Apex TruVis Esters™ 810TM N-C8C10 Trimellitate |
|||
Specific Gravity | 0.978 g/cc | 0.978 g/cc | ASTM D792 |
PolyOne Elastamax™ XL-0153-24 Styrene Butadiene Block Copolymer (SBC)
(discontinued **) A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in acco.. |