Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.956 g/cc | 0.956 g/cc | ISO 1183 |
Polimeri Europa Eraclene® MM 84 High Density Polyethylene - Injection Molding Eraclene MM 84 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MM 84 is characterized by high rigidity and good impact resistance. .. |
|||
Specific Gravity | 0.956 g/cc | 0.956 g/cc | ISO 1183 |
SCG Chemicals EL-Leneâ„¢ H5211PBL High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stability, good resistance to weatheringRecommended Applications: Stripe lines for PE80 pipe, non pressure pipesCertification: Certified by LNEI.. |
|||
Specific Gravity | 0.956 g/cc | 0.956 g/cc | ASTM D1505 |
SCG Chemicals EL-Leneâ„¢ H5604F High Density Polyethylene Film Key Characteristics:High tensile strengthHigh dart impactHigh stiffnessLow gel contentGood moisture barrierRecommended Applications: Films for shopping bag, T-shirt bag, garbage bag, liner bagInfor.. |
|||
Specific Gravity | 0.956 g/cc | 0.956 g/cc | ASTM D1505 |
SCG Chemicals EL-Leneâ„¢ H5615F High Density Polyethylene Film Key Characteristics:High speed processingHigh tensile strengthHigh dart impactLow gel contentGood moisture barrierRecommended Applications: Ultra thin film ( |
|||
Specific Gravity | 0.956 g/cc @Temperature 25.0 °C |
0.956 g/cc @Temperature 77.0 °F |
|
Dow Corning 3225C Formulation Aid Dispersion of high molecular weight silicone surfactant in volatile dimethylsiloxane, designed to prepare water-in-silicone emulsions.Information provided by Dow Corning |
|||
Specific Gravity | 0.956 g/cc @Temperature 25.0 °C |
0.956 g/cc @Temperature 77.0 °F |
|
Dow Corning 5225C Formulation Aid A 10% dispersion of high molecular weight silicone polyether in cyclopentasiloxane fluid for use in skincare, suncare, hair care, color cosmetic, and antiperspirant / deodorant applications. INCI Na.. |
|||
Specific Gravity | 0.956 g/cc | 0.956 g/cc | ASTM D792 |
Braskem Green PE SHA7260 Injection Molding High Density Polyethylene Description: SHA7260 is a high-density polyethylene, developed for the injection molding, easy to process and with high productivity. This resin has a good melt flow with high rigidity and hardness... |
|||
Specific Gravity | 0.956 g/cc | 0.956 g/cc | ASTM D792 |
Braskem Green PE SGF4950 Blow Molding and Monofilament High Density Polyethylene Description: SGF4950 is a high-density polyethylene copolymer, developed for the blow-molding segment. It shows well balanced properties between impact and stiffness, combined with high environmenta.. |
|||
Specific Gravity | 0.956 g/cc | 0.956 g/cc | ISO 1183 |
Polimeri Europa Eraclene® MM 84 U High Density Polyethylene - Injection Molding Eraclene MM 84 U is a gas phase high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MM 84 U is characterized by high rigidity and good impac.. |