Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.940 g/cc | 0.940 g/cc | ASTM D792 |
Polimeri Europa Europrene® SOL T 161C Styrene - Butadiene Block Copolymer Europrene® SOL T 161C is a radial block copolymer obtained by anionic polymerization. The polymer is based on styrene and butadiene, where bound styrene is 30% weight. A non-staining antioxidant .. |
|||
Specific Gravity | 0.940 g/cc | 0.940 g/cc | ASTM D792 |
Quadrant EPP TIVAR® Dockguard - UHMW-PE - Black UV Stabilized UHMW-PE (ASTM Product Data Sheet) |
|||
Specific Gravity | 0.940 g/cc | 0.940 g/cc | ISO 2781 |
LG Chemical LG-428N Styrene-Butadiene-Styrene Description: Radial structure, Non-Oil Extended Grade Thermoplastic ElastomerApplications: Asphalt Modifier, Plastic Modifier, Compounding, Adhesives etcCAS: 9003-55-8Information provided by LG Chem.. |
|||
Specific Gravity | 0.940 g/cc | 0.940 g/cc | |
LG Chemical SBR 1500 High Acrylonitrile Polymer Description: NSBR 1500 is a cold polymerized styrene-butadiene copolymer with staining stabilizer. The cold polymerized SBR exhibits better abrasion, higher tensile strength and higher modulus than .. |
|||
Specific Gravity | 0.940 g/cc | 0.940 g/cc | ASTM D792 |
Micropol Microcoat DG/EVA/214A Microground modified EVA copolymer Specially developed for high specification coating where metal/coating adhesion is of primary importance. Typically used on large flat surfaces, and when toughness, elasticity and excellent barrier .. |
|||
Specific Gravity | 0.940 g/cc | 0.940 g/cc | ISO 2781 |
Kraton® D1101 E (SBS) Liner Block Copolymer Description: Kraton D1101 E polymer is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 31% mass. It is supplied from Europe in the physical forms identified as f.. |
|||
Specific Gravity | 0.940 g/cc | 0.940 g/cc | ISO 2781 |
Kraton® D1189 E (SBS) Radial Block Copolymer Description: Kraton D1189 E is a clear, radial block copolymer based on styrene and butadiene with bound styrene of 32% mass. It is supplied from Europe in the physical forms indicated in the grade .. |
|||
Specific Gravity | 0.940 g/cc | 0.940 g/cc | ASTM D792 |
Kraton® D4153 E (O/E SBS) Linear Block Copolymer Description: Kraton D4153 E is an oil-extended linear block copolymer based on styrene and butadiene with bound styrene in the neat polymer of 35% mass. It contains 40 phr paraffinic oil which is cl.. |
|||
Specific Gravity | 0.940 g/cc | 0.940 g/cc | 15.5/15.5°C |
LG Chemical C9 Product Physical Properties: Colorless liquid similar to DIESEL oilObtained as a by-product from pyrolysis oil hydration plant which was produced from naphtha pyrolysis process. It is composed of hydrocarbo.. |
|||
Specific Gravity | 0.940 g/cc | 0.940 g/cc | ASTM D792 |
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 40-LR-1 TPE Product Description: StarTUFF TF 40-LR-1 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M.. |
|||
Specific Gravity | 0.940 g/cc | 0.940 g/cc | ASTM D792 |
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 40-LR-9 TPE Product Description: StarTUFF TF 40-LR-9 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M.. |
|||
Specific Gravity | 0.940 g/cc | 0.940 g/cc | ASTM D792 |
Teknor Apex Telcar® TL-6065 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Specific Gravity | 0.940 g/cc | 0.940 g/cc | ASTM D792 |
Teknor Apex Telcar® TL-6800-73 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Specific Gravity | 0.940 g/cc | 0.940 g/cc | ASTM D792 |
Teknor Apex UNIPRENE® 7100-73 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Specific Gravity | 0.940 g/cc | 0.940 g/cc | ASTM D792 |
Teknor Apex Uniprene® UN-1069A Thermoplastic Elastomer Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Specific Gravity | 0.940 g/cc | 0.940 g/cc | ISO 1183/1 |
A. Schulman FORMION™ FI 391 Ionomer DescriptionFormion® FI 391 is a non-reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low temperature ductility, and medium stiffness. Formion F1 391U i.. |
|||
Specific Gravity | 0.940 g/cc | 0.940 g/cc | ISO 1183/1 |
A. Schulman FORMION™ FI 105 Non-Reinforced, Injection Molding Grade Sodium Ionomer DescriptionFormion® FI 105 is a non-reinforced, transparent, injection molding grade Sodium Ionomer. It has been formulated for high durability, scratch resistance, low temperature ductility, and .. |
|||
Specific Gravity | 0.940 g/cc | 0.940 g/cc | ISO 1183/1 |
A. Schulman FORMION™ FI 391 Ionomer DescriptionFormion® FI 391 is a non-reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low temperature ductility, and medium stiffness. Formion F1 391U i.. |
|||
Specific Gravity | 0.940 g/cc | 0.940 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ AF-1085 Antifog Concentrate DescriptionPOLYBATCH® AF-1085 is a 10% antifog concentrate based in LDPE. This concentrate is designed to provide excellent antifog performance in polyethylene film applications ranging from meat .. |
|||
Specific Gravity | 0.940 g/cc | 0.940 g/cc | ASTM D792 |
A. Schulman LP552-01 Injection Molding, Extrusion Grade Compound DescriptionLP 522-01 is an injection molding and/or extrusion grade compoundApplicationLP 552-01 meets FDA Regulation CFT 177.1520(c)3.1.Information provided by A. Schulman. |
|||
Specific Gravity | 0.940 g/cc | 0.940 g/cc | ISO 1183/1 |
A. Schulman FORMION™ FI 391 Ionomer DescriptionFormion® FI 391 is a non-reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low temperature ductility, and medium stiffness. Formion F1 391U i.. |
|||
Specific Gravity | 0.940 g/cc | 0.940 g/cc | ISO 1183/1 |
A. Schulman FORMION™ FI 105E Non-Reinforced, Extrusion Grade Sodium Ionomer DescriptionFormion® FI 1051E is a non-reinforced, transparent, extrusion grade Sodium Ionomer. It has been formulated for high durability, cut and puncture resistance, and low temperature ductilit.. |
|||
Specific Gravity | 0.940 g/cc | 0.940 g/cc | ISO 1183 |
Total EVA 1005 VN 5 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1005 VN 5 is made by a high pressure tubular process. Grade for films with high transparency and good mechanical properties. Contains an antioxidant.Application examples: Coextrusion, stretch .. |
|||
Specific Gravity | 0.940 g/cc | 0.940 g/cc | ISO 1183/1 |
A. Schulman FORMION™ FI 391 Ionomer DescriptionFormion® FI 391 is a non-reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low temperature ductility, and medium stiffness. Formion F1 391U i.. |
|||
Specific Gravity | 0.940 g/cc @Temperature 25.0 °C |
0.940 g/cc @Temperature 77.0 °F |
|
Dow Corning Z-6187 SILANE Dow Corning® Z-6187 Silane is a dialkyldimethoxysilane. Silanes and siloxanes have been used for some time in this application to increase yield and improve the stereoregularity of the polyolefin r.. |
|||
Specific Gravity | 0.940 g/cc | 0.940 g/cc | |
Dow Corning Z-6690 WATER REPELLENT Dow Corning® Z-6690 Water Repellent is a solvent-free silane/ siloxane concentrate that can be diluted in organic or silicone solvents to formulate water repellents. Upon application of the diluted.. |
|||
Specific Gravity | 0.940 g/cc | 0.940 g/cc | ASTM D792 |
Chi Mei Kibiton® PB-5300 SBC Compounding, transparent goods |
|||
Specific Gravity | 0.940 g/cc | 0.940 g/cc | 23°C; ASTM D792 |
ExxonMobil Santoprene® 8201-90 Thermoplastic Elastomer A hard, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |
|||
Specific Gravity | 0.940 g/cc | 0.940 g/cc | ISO 2782 |
AlphaGary Evoprene™ G 966 SEBS Thermoplastic Elastomer Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi.. |