Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.730 g/cc | 0.730 g/cc | |
Permabond ASC10 Anaerobic Surface Conditioner PERMABOND ASC10 Anaerobic Conditioner is a rapid drying accelerator for use with PERMABOND Anaerobic Adhesive/Sealants. It is designed to be used primarily on inactive surfaces such as zinc plating,.. |
|||
Specific Gravity | 0.730 g/cc | 0.730 g/cc | |
Permabond QFS16 Cyanoacrylate Activator The PERMABOND QFS 16 accelerates the cure of cyanoacrylate adhesives to provide a shorter set time. It can be used in a variety of applications but is especially useful when bonding porous or poorly.. |
|||
Specific Gravity | 0.730 g/cc | 0.730 g/cc | |
Shin-Etsu Silicones X-33-156-20 Silicone Primer Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Specific Gravity | 0.730 g/cc | 0.730 g/cc | |
Shin-Etsu Silicones X-33-173AB Silicone Primer Information Provided by Shin-Etsu Silicones of America, Inc. |