Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.560 g/cc | 0.560 g/cc | Part B; TM R050-16 |
Resinlab® EP1287 Filled, Flame Retardant Epoxy Syntactic Foam Resinlab™ EP1287 is a two part filled, flame retardant epoxy syntactic foam. It utilizes glass microspheres to reduce cured density and improve machinability. This product will be self-extinguishin.. |
|||
Specific Gravity | 0.560 - 0.720 g/cc | 0.560 - 0.720 g/cc | |
Cos70 Cork/Synthetic Rubber Sheet Description: Harvested every 9-12 years from the cork oak tree, cork is able to rebound from compression with extrusion. Applications include: stoppers, soundproofing, flooring, gaskets, and many ot.. |
|||
Specific Gravity | 0.560 g/cc | 0.560 g/cc | ASTM D3574 |
Azdel SuperLite® SL550700-100 PP Resin Matrix / 55% Glass Fiber (1.5 mm Molded Thickness) AZDEL SuperLite® SL550700-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |