Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 3.75 - 4.25 g/cc | 3.75 - 4.25 g/cc | |
Parker Chomerics CHO-SEAL 1240 Conductive Elastomer Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics |
|||
Specific Gravity | 3.75 - 4.25 g/cc | 3.75 - 4.25 g/cc | |
Parker Chomerics CHO-SEAL 1278 Conductive Elastomer Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics |