Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.95 - 2.45 g/cc | 1.95 - 2.45 g/cc | ASTM D792 |
Parker Chomerics CHO-BOND® 1016 Electrically Conductive Sealant Description: CHO-BOND 1016 sealant is an electrically conductive, one-component RTV silicone which provides both environmental sealing and EMI shielding. This seal, filled with nickel-plated graphit.. |
|||
Specific Gravity | 1.95 - 2.45 g/cc | 1.95 - 2.45 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL L6303 Conductive Elastomer Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Molded and ExtrudedRoHS CompliantInformation provid.. |
|||
Specific Gravity | 2.30 - 2.45 g/cc | 2.30 - 2.45 g/cc | ISO 1183 |
Raschig Group EN 5004 Epoxy Molding Compound Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo.. |
|||
Specific Gravity | 2.30 - 2.45 g/cc | 2.30 - 2.45 g/cc | ISO 1183 |
Raschig Group EN 5007 Epoxy Molding Compound Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo.. |