Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.55 - 2.05 g/cc | 1.55 - 2.05 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL 6309 Extruded Elastomer Commercial Grade Extruded Elastomer. This is an extruded nickel-plated graphite filled silicone elastomer that provides a minimum shielding effectiveness of 75 dB from 100 MHz to 10 GHz. This low co.. |
|||
Specific Gravity | 1.55 - 2.05 g/cc | 1.55 - 2.05 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL® 6310 Extruded Elastomer Low Cost Commercial Grade Extruded Elastomer. CHO-SEAL 6310 is the latest addition to Chomerics line of low cost, commercial grade EMI gaskets. This extruded material combines nickel-plated graphite.. |
|||
Specific Gravity | 1.55 - 2.05 g/cc | 1.55 - 2.05 g/cc | |
Parker Chomerics CHO-SEAL® 6315 Graphite Filled Elastomer EMI Gaskets. This extruded nickel-plated graphite filled elastomer addresses EMI shielding and environmental needs for both internal and external applications. It has an excellent performance in sal.. |
|||
Specific Gravity | 1.55 - 2.05 g/cc | 1.55 - 2.05 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL® 6372 Graphite Filled Elastomer EMI Gaskets. This extruded nickel-plated graphite filled elastomer addresses EMI shielding and environmental needs for both internal and external applications. It has an excellent performance in sal.. |
|||
Specific Gravity | 1.55 - 2.05 g/cc | 1.55 - 2.05 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL® 6510 Conductive Elastomer Extruded onlyInformation provided by Chomerics |
|||
Specific Gravity | 1.55 - 2.05 g/cc | 1.55 - 2.05 g/cc | ASTM D792 |
Parker Chomerics Tecknit Consil®-II 841 Molded Silver-Filled Silicone Elastomer Description: CONSIL-II is a molded silicone elastomer filled with silver-coated inert particles. It provides high electrical conductivity, broadband shielding and moisture sealing. CONSIL-II is desi.. |
|||
Specific Gravity | 1.95 - 2.05 g/cc | 1.95 - 2.05 g/cc | ISO 1183 |
Raschig Group 3536 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed.. |
|||
Specific Gravity | 1.55 - 2.05 g/cc | 1.55 - 2.05 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL 1310 Conductive Elastomer Moderate performance in non-corrosive environments, no corrosion or fluid resistance; material of choice for small, delicate injection-molded parts or large dimension extrusionsMolded onlyRoHS Compl.. |
|||
Specific Gravity | 2.03 - 2.05 g/cc | 2.03 - 2.05 g/cc | ASTM D792 |
Adamas Adalon® 125 PTFE, 35% Carbon Filled Information provided by Adamas, HPM |
|||
Specific Gravity | 1.95 - 2.05 g/cc | 1.95 - 2.05 g/cc | ASTM D792 |
Adamas Adalon® 401 PTFE, 10% Polyimide Information provided by Adamas, HPM |
|||
Specific Gravity | 1.95 - 2.05 g/cc | 1.95 - 2.05 g/cc | ASTM D792 |
Adamas Adalon® 433 PTFE, 10% Ekonol® Information provided by Adamas, HPM |
|||
Specific Gravity | 1.90 - 2.05 g/cc | 1.90 - 2.05 g/cc | |
Bulk Molding Compounds BMC 102 Glass Filled Thermoset Polyester BMC 102 is a medium strength, glass fiber reinforced molding compound that meets Ford Specification ESF-M3D56-A. It can be supplied in bulk or extruded in pre-weighed slugs and is well suited for in.. |
|||
Specific Gravity | 1.75 - 2.05 g/cc | 1.75 - 2.05 g/cc | |
Bulk Molding Compounds BMC 304 Automotive Grade Molding Compound BMC 304 is a low profile, automotive grade molding compound that is suitable for Injection, Compression or Transfer molding operations. BMC 304 can be coated using traditional or electrostatic coati.. |
|||
Specific Gravity | 1.75 - 2.05 g/cc | 1.75 - 2.05 g/cc | |
Bulk Molding Compounds BMC 606 Mineral Filled, Glass Reinforced Polyester Compound BMC 606 is a mineral filled, glass reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good moldability, excellent impact strength,.. |
|||
Specific Gravity | 1.95 - 2.05 g/cc | 1.95 - 2.05 g/cc | |
Bulk Molding Compounds BMC 1050 Thermoset Polyester BMC 1050 is a cosmetic, appliance grade material with superior heat stability. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.Typical applications are toaster e.. |
|||
Specific Gravity | 1.75 - 2.05 g/cc | 1.75 - 2.05 g/cc | |
Bulk Molding Compounds BMC 300 Mineral Filled, Glass Reinforced Polyester BMC 300 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. Our Granite-X series of molding compounds bel.. |