Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.93 - 1.96 g/cc | 1.93 - 1.96 g/cc | ASTM D792 |
Adamas Adalon® 406 PTFE, 15% PEEK Information provided by Adamas, HPM |
|||
Specific Gravity | 1.90 - 1.96 g/cc | 1.90 - 1.96 g/cc | |
3M Dyneon™ Dynamar™ FX 5911 Polymer Processing Additive Dynamar FX 5911 is a free-flowing fluoropolymer processing aid that is designed for use at very low levels (typically 250-1000 ppm) necessary to improve processing, it does not alter or detract from.. |
|||
Specific Gravity | 1.90 - 1.96 g/cc | 1.90 - 1.96 g/cc | |
3M Dyneon™ FX 5912 Dynamar™ Polymer Processing Additive Dynamar FX 5912 is a free-flowing fluorothermoplastic processing aid that is designed for use at very low levels to improve the processing of thermoplastics. Typical use levels of 200 to 1000 ppm ha.. |
|||
Specific Gravity | 1.88 - 1.96 g/cc | 1.88 - 1.96 g/cc | |
Bulk Molding Compounds BMC 605LS Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 605LS molding compound is a low-shrink, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is characterized by good mol.. |
|||
Specific Gravity | 1.93 - 1.96 g/cc | 1.93 - 1.96 g/cc | ASTM D792 |
Adamas Adalon® 477 PTFE, 20% Aramid Fiber Information provided by Adamas, HPM |