Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.65 - 1.69 g/cc | 1.65 - 1.69 g/cc | ASTM D-792 |
Axiall 02540 Plenum Flexible PVC Non-lead stabilized Category 3 plenum jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |