Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.47 - 1.53 g/cc | 1.47 - 1.53 g/cc | ASTM D 792 |
Karina E831-28/16-Y-ERYB-LMP Cool Gray PVC Compound Heavy metal free PVC compound recommended for extrusion of furniture profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.47 - 1.53 g/cc | 1.47 - 1.53 g/cc | ASTM D 792 |
Karina Karintox 70 Polyolefin Compound Halogen free, fire retardant, low smoke and fume polyolefinic compound. Recommended for insulation of electrical cables up to 1KV.Information provided by Karina Indústria e Comércio de Plá.. |
|||
Specific Gravity | 1.47 - 1.53 g/cc | 1.47 - 1.53 g/cc | NBR NM-IEC 60811-1-3 |
Karina 02/284-FC-LMP Yellow Color Concentrate for PVC Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.47 - 1.53 g/cc | 1.47 - 1.53 g/cc | ASTM D 792 |
Karina 06/183-RG-GE (CS) Blue Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.47 - 1.53 g/cc | 1.47 - 1.53 g/cc | ASTM D 792 |
Karina 18/335-FC Gray Color Concentrate for PVC Color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. Recommended to use.. |
|||
Specific Gravity | 1.47 - 1.53 g/cc | 1.47 - 1.53 g/cc | NBR NM-IEC 60811-1-3 |
Karina 18/335-FC-LMP Gray Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.47 - 1.53 g/cc | 1.47 - 1.53 g/cc | NBR NM-IEC 60811-1-3 |
Karina 32/1-FC-LMP Orange Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.47 - 1.53 g/cc | 1.47 - 1.53 g/cc | ASTM D 792 |
Karina 32/82-FC-(CS) Orange Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.47 - 1.53 g/cc | 1.47 - 1.53 g/cc | ASTM 792 |
Karina 806-10/236-H-ISE White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.47 - 1.53 g/cc | 1.47 - 1.53 g/cc | ASTM D 792 |
Karina 806-18/364-BY-ERYB Gray PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.47 - 1.53 g/cc | 1.47 - 1.53 g/cc | ASTM D 792 |
Karina 806-40/236-H-ISE-LMP White PVC Compound Heavy metal free PVC compound.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.47 - 1.53 g/cc | 1.47 - 1.53 g/cc | ASTM D 792 |
Karina 806-48/1-H-ISE-LMP Black PVC Compound Heavy metal free PVC compound.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.47 - 1.53 g/cc | 1.47 - 1.53 g/cc | ASTM D 792 |
Karina 807-10/236-H-Ise White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.47 - 1.53 g/cc | 1.47 - 1.53 g/cc | NBR 14288 |
Karina 828-08/20-AY-ERYB Beige PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.47 - 1.53 g/cc | 1.47 - 1.53 g/cc | NBR 14288 |
Karina 828-08/20-AY-ERYB-PO Beige PVC Compound PVC powder compound recommended for extrusion in twin screw extruder of door profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.47 - 1.53 g/cc | 1.47 - 1.53 g/cc | ASTM D 792 |
Karina 828-28/14-AY-ERYB Ice (Light Gray) PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.47 - 1.53 g/cc | 1.47 - 1.53 g/cc | ASTM D 792 |
Karina 830-48/1-AY-ERYB Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.47 - 1.53 g/cc | 1.47 - 1.53 g/cc | ASTM D 792 |
Karina 850-10/116-Y-ERYB-AS White PVC Compound PVC powder compound recommended for extrusion in twin screw extruder of window profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.47 - 1.53 g/cc | 1.47 - 1.53 g/cc | ASTM D 792 |
Karina 850-10/99-Y-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.47 - 1.53 g/cc | 1.47 - 1.53 g/cc | ASTM D 792 |
Karina E 08/244-RG-GE Beige Color Concentrate for PVC Color concentrate recommended for application in rigid PVC compounds for general purposes. Important Considerations:Heavy metal freeFormulated with inorganic pigments PVC resin based (carrier polyme.. |
|||
Specific Gravity | 1.47 - 1.53 g/cc | 1.47 - 1.53 g/cc | NBR NM-IEC 60811-1-3 |
Karina E 10/85-FC-LMP White Color Concentrate for PVC Color concentrate recommended for application in PVC compounds for electrical wires and cables. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes.Important con.. |
|||
Specific Gravity | 1.47 - 1.53 g/cc | 1.47 - 1.53 g/cc | NBR NM-IEC 60811-1-3 |
Karina E 32/1-FC-LMP Orange Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.47 - 1.53 g/cc | 1.47 - 1.53 g/cc | ASTM D 792 |
Karina E 36/287-GIN Gold Brown MB (SP31467) for PVC Recommended usage from 2% to 3% on crystal PVC compoundInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.47 - 1.53 g/cc | 1.47 - 1.53 g/cc | ASTM D 792 |
Karina E 813-10/369-BY-ERYB White PVC Compound Rigid PVC compound recommended to extrude general profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.47 - 1.53 g/cc | 1.47 - 1.53 g/cc | NBR NM-IEC 60811-1-3 |
Karina 40/14-FC-LMP Green Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.47 - 1.53 g/cc | 1.47 - 1.53 g/cc | ASTM D 792 |
Karina 39/47-FC-LMP Pink Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.47 - 1.53 g/cc | 1.47 - 1.53 g/cc | NBR 14288 |
Karina 802-10/55-AY-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.47 - 1.53 g/cc | 1.47 - 1.53 g/cc | NBR 14288 |
Karina 802-10/93-AY-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |