Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.00 - 1.05 g/cc | 1.00 - 1.05 g/cc | LSY-QB-ID002 |
LG Chemical Lutex 703 SBR Latex Description: Binding Force, Ink set off, Post Treatment Properties, Coater RunnabilityApplication: Art Paper, Paperboard-Single, Pre-Rod, Blade Coater, Adhesive coated paper and Carpet back-coating .. |
|||
Specific Gravity | 1.00 - 1.05 g/cc | 1.00 - 1.05 g/cc | LSY-QB-ID002 |
LG Chemical Lutex 704 SBR Latex Description: Binding Force, Print gloss, High Shear Rheology, Coater RunnabilityApplication: Art Paper-Single, Pre-Film, Blade Coater, Adhesive coated paper and Carpet back-coating adhesiveCSA No. 7.. |
|||
Specific Gravity | 1.00 - 1.05 g/cc | 1.00 - 1.05 g/cc | LSY-QB-ID002 |
LG Chemical Lutex 760 SBR Latex Description: Binding Force, Print gloss, High Shear Rheology, Post Treatment Properties, Coater RunnabilityApplication: Art Paper, Paperboard-Single, Top-Film, Blade Coater, Adhesive coated paper an.. |
|||
Specific Gravity | 1.00 - 1.05 g/cc | 1.00 - 1.05 g/cc | LSY-QB-ID002 |
LG Chemical Lutex 810 SBR Latex Description: Blister Resistance, Ink set off, Sheet Gloss, Coater RunnabilityApplication: Art Paper, Web Offset, Blade Coater and Adhesive coated paperCSA No. 70857-13-5 and 7732-18-5Information pro.. |
|||
Specific Gravity | 1.00 - 1.05 g/cc | 1.00 - 1.05 g/cc | LSY-QB-ID002 |
LG Chemical Lutex M710 SBR Latex Description: High Binding Force (MSP), Ink set off, Print Mottle, Coater RunnabilityApplication: Art Paper, Paperboard-Single, Top-Film Coater, Adhesive coated paper and Carpet back-coating adhesive.. |
|||
Specific Gravity | 1.03 - 1.05 g/cc | 1.03 - 1.05 g/cc | |
Michelman® Michem® Flex P1850 Water based primer Description: Water based primer for liquids and extrusion coated resins.Usage: Michem® Flex P1850 is a primer for film, metal and paper substrates to promote adhesion to extrusion coated resins r.. |
|||
Specific Gravity | 1.03 - 1.05 g/cc | 1.03 - 1.05 g/cc | |
Michelman® Micryl™ 766R Water resistant coating Description: General purpose water resistant coatingUsage: Micryl™ 766R is a water and grease resistant coating that can also function as a heat resistant gloss overprint. In such applications,.. |
|||
Specific Gravity | 1.03 - 1.05 g/cc | 1.03 - 1.05 g/cc | |
Samsung Cheil Industries Starex® SF-100H Expandable Polystyrene (EPS) FR Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.03 - 1.05 g/cc | 1.03 - 1.05 g/cc | |
Samsung Cheil Industries Starex® SF-101H Expandable Polystyrene (EPS) FR Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.03 - 1.05 g/cc | 1.03 - 1.05 g/cc | |
Samsung Cheil Industries Starex® SF-200H Expandable Polystyrene (EPS) FR Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.03 - 1.05 g/cc | 1.03 - 1.05 g/cc | |
Samsung Cheil Industries Starex® SF-400H Expandable Polystyrene (EPS) FR Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.03 - 1.05 g/cc | 1.03 - 1.05 g/cc | |
Samsung Cheil Industries Starex® SG-101 Expandable Polystyrene (EPS) High Expansion Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.03 - 1.05 g/cc | 1.03 - 1.05 g/cc | |
Samsung Cheil Industries Starex® SG-201 Expandable Polystyrene (EPS) High Expansion Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.03 - 1.05 g/cc | 1.03 - 1.05 g/cc | |
Samsung Cheil Industries Starex® SG-202 Expandable Polystyrene (EPS) High Expansion Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.03 - 1.05 g/cc | 1.03 - 1.05 g/cc | |
Samsung Cheil Industries Starex® SG-301 Expandable Polystyrene (EPS) High Expansion Typical Application : Large FloatInformation provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.03 - 1.05 g/cc | 1.03 - 1.05 g/cc | |
Samsung Cheil Industries Starex® SG-302 Expandable Polystyrene (EPS) High Expansion Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.03 - 1.05 g/cc | 1.03 - 1.05 g/cc | |
Samsung Cheil Industries Starex® SG-401 Expandable Polystyrene (EPS) High Expansion Typical Application : Large FloatInformation provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.03 - 1.05 g/cc | 1.03 - 1.05 g/cc | |
Samsung Cheil Industries Starex® SF-100H Expandable Polystyrene (EPS) FR Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.03 - 1.05 g/cc | 1.03 - 1.05 g/cc | |
Samsung Cheil Industries Starex® SF-101H Expandable Polystyrene (EPS) FR Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.03 - 1.05 g/cc | 1.03 - 1.05 g/cc | |
Samsung Cheil Industries Starex® SF-200H Expandable Polystyrene (EPS) FR Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.03 - 1.05 g/cc | 1.03 - 1.05 g/cc | |
Samsung Cheil Industries Starex® SF-300H Expandable Polystyrene (EPS) FR Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.03 - 1.05 g/cc | 1.03 - 1.05 g/cc | |
Samsung Cheil Industries Starex® SF-301H Expandable Polystyrene (EPS) FR Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.03 - 1.05 g/cc | 1.03 - 1.05 g/cc | |
Samsung Cheil Industries Starex® SF-400H Expandable Polystyrene (EPS) FR Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.03 - 1.05 g/cc | 1.03 - 1.05 g/cc | |
Samsung Cheil Industries Starex® SG-201 Expandable Polystyrene (EPS) High Expansion Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.03 - 1.05 g/cc | 1.03 - 1.05 g/cc | |
Samsung Cheil Industries Starex® SG-301 Expandable Polystyrene (EPS) High Expansion Typical Application : Large FloatInformation provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.03 - 1.05 g/cc | 1.03 - 1.05 g/cc | |
Samsung Cheil Industries Starex® SG-302 Expandable Polystyrene (EPS) High Expansion Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.03 - 1.05 g/cc | 1.03 - 1.05 g/cc | |
Samsung Cheil Industries Starex® SG-401 Expandable Polystyrene (EPS) High Expansion Typical Application : Large FloatInformation provided by Samsung Cheil Industries. |
|||
Specific Gravity | 0.950 - 1.05 g/cc | 0.950 - 1.05 g/cc | |
Chesterton 630 SXCF Synthetic, Extreme Pressure & Corrosion Resistant Grease Description: Superior resistance to washout by water, caustics, sanitizing cleaners, process fluids and steam has now been combined with high temperature performance to product Chesterton® 630 SXCF.. |
|||
Specific Gravity | 0.970 - 1.05 g/cc | 0.970 - 1.05 g/cc | ASTM D792 |
Buckeye Polymers BP RPP 1310 T NAT Polypropylene, Talc Filled Product Information: Our Talc filled product lines exhibit excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and .. |
|||
Specific Gravity | 0.950 - 1.05 g/cc | 0.950 - 1.05 g/cc | |
Chesterton 633 SXCM Synthetic, Extreme Pressure & Corrosion Resistant Grease-with Moly Description: Chesterton® 633 Synthetic Extreme Pressure & Corrosion Resistant Grease with Moly is the one grease to use for the most demanding lubricating needs. It is a multi-purpose workhorse wit.. |