Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 7.41 g/cc | 7.41 g/cc | |
Latrobe DuraTechâ„¢ NINE Powder Metal Tool Steel DuraTech NINE is an air-hardening, powder metal tool steel that provides very high wear resistance in combination with high impact toughness. A large volume of hard vanadium carbides provides the hi.. |
|||
Specific Gravity | 7.41 g/cc | 7.41 g/cc | |
Latrobe DuraTech™ A11 Powder Metal Tool Steel (AISI A11) DuraTech A11 powder metal tool steel a versatile air-hardening tool and die steel which provides extremely high wear resistance in combination with relatively high impact toughness. A very large vol.. |