Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 7.00 g/cc | 7.00 g/cc | |
Silberline Silcroma® BG-15 Silcroma® products are iron flake pigments that have been treated to impart a black color to the flake surface. The black color is an integral part of the flake and will not bleed during processi.. |
|||
Specific Gravity | 7.00 g/cc | 7.00 g/cc | |
Silberline Silcroma® BG-13 Silcroma® products are iron flake pigments that have been treated to impart a black color to the flake surface. The black color is an integral part of the flake and will not bleed during processi.. |
|||
Specific Gravity | 7.00 g/cc | 7.00 g/cc | ASTM D792 |
Ecomass® 720ZD91 Tungsten Filled ABS High Specific GravityTungsten Powder Filled ABSGood ToughnessPlateableInformation provided by Technical Polymers |